Determination of impurity elements Si,Mn,Mg,Cu,Zn,Cd,Pb,and Zr in nickel lanthanum alloy by inductively coupled plasma atomic emission spectrometry
Avic Beijing
Abstract
Avic Beijing
Abstract
A method for determination of impurity elements in nickel lanthanum alloy by inductively coupled plasma atomic emission spectrometry(ICP-AES)was proposed.All the influencing factors on spectrum measuring were investigated.The sample was decomposed by mixed acid(HCL,HNO3),the experiment of instrument parameters,selection of analysis lines were studied,the optimal determination conditions of instrument were obtained,the analytical lines were Si 251.611 nm,Mn 257.610 nm,Mg285.213 nm,Cu 324.752 nm,Zn 213.857 nm,Cd 214.440 nm,Pb 220.353 nm,Zr 343.823 nm,respectively,the effect of matrix and coexist elements on the determination was carried out.The matrix effect was corrected by matrix matching.The detection limits were 0.0003-0.015μg/ml,the recovery rates were from 80%to 108%,the RSD were less than 8%.
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
A method for determination of impurity elements in nickel lanthanum alloy by inductively coupled plasma atomic emission spectrometry(ICP-AES)was proposed.All the influencing factors on spectrum measuring were investigated.The sample was decomposed by mixed acid(HCL,HNO3),the experiment of instrument parameters,selection of analysis lines were studied,the optimal determination conditions of instrument were obtained,the analytical lines were Si 251.611 nm,Mn 257.610 nm,Mg285.213 nm,Cu 324.752 nm,Zn 213.857 nm,Cd 214.440 nm,Pb 220.353 nm,Zr 343.823 nm,respectively,the effect of matrix and coexist elements on the determination was carried out.The matrix effect was corrected by matrix matching.The detection limits were 0.0003-0.015μg/ml,the recovery rates were from 80%to 108%,the RSD were less than 8%.
Key concepts: Lanthanum, Inductively coupled plasma, Analytical Chemistry (journal), Impurity, Nickel, Inductively coupled plasma atomic emission spectroscopy, Matrix (chemical analysis), Alloy