Study on the wear resistance of three carburizing structural steel after different chemico-thermal treatment

Jinping Li

Open publisher page 0 citations

Abstract

The wear resistance of 18Cr2Ni4WA,27SiMnMoV and 25SiCrMoV steel after carburizing ,carbonitriding and nitriding trearment is studied.The results show that the wear resistance of 25SiCrMoV steel is the best and that of 18Cr2Ni4WA steel is the worst after three different chemico-thermal treatment.

About this research paper

What this paper is about

The wear resistance of 18Cr2Ni4WA,27SiMnMoV and 25SiCrMoV steel after carburizing ,carbonitriding and nitriding trearment is studied.The results show that the wear resistance of 25SiCrMoV steel is the best and that of 18Cr2Ni4WA steel is the worst after three different chemico-thermal treatment.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The wear resistance of 18Cr2Ni4WA,27SiMnMoV and 25SiCrMoV steel after carburizing ,carbonitriding and nitriding trearment is studied.The results show that the wear resistance of 25SiCrMoV steel is the best and that of 18Cr2Ni4WA steel is the worst after three different chemico-thermal treatment.

Key concepts: Carburizing, Carbonitriding, Nitriding, Wear resistance, Metallurgy, Materials science, Thermal treatment, Thermal

Related papers

Back to paper searchBrowse research topicsOriginal source
Study on the wear resistance of three carburizing structural steel after different chemico-thermal treatment — Research Paper | ScholarLens