2005Journal of University of Science and Technology BeijingRequires access

Deep dephosphorization ability of BaO-CaO-CaF_2 flux for liquid steel

Lixin Zhu

Open publisher page 1 citations

Abstract

Deep dephosphorization experiment was carried out in the laboratory by BaO-CaO-CaF2 flux to obtain ultra-low phosphorus steel. The result showed that the P content of the tested steel could decrease from about 0.01% to 0.005% or even lower to 0.002% with a dephosphorization ratio of 50% by use of this kind of flux. It is found that the oxidizability of steel has significant effect on dephosphoriztion when using the BaO-CaO-CaF2 flux. The phosphate capacity of the used system varied from 1018 to 1019.35 in 1 813-1 893 K and increased with the increasing of BaO content.

About this research paper

What this paper is about

Deep dephosphorization experiment was carried out in the laboratory by BaO-CaO-CaF2 flux to obtain ultra-low phosphorus steel. The result showed that the P content of the tested steel could decrease from about 0.01% to 0.005% or even lower to 0.002% with a dephosphorization ratio of 50% by use of this kind of flux. It is found that the oxidizability of steel has significant effect on dephosphoriztion when using the BaO-CaO-CaF2 flux. The phosphate capacity of the used system varied from 1018 to 1019.35 in 1 813-1 893 K and increased with the increasing of BaO content.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Deep dephosphorization experiment was carried out in the laboratory by BaO-CaO-CaF2 flux to obtain ultra-low phosphorus steel. The result showed that the P content of the tested steel could decrease from about 0.01% to 0.005% or even lower to 0.002% with a dephosphorization ratio of 50% by use of this kind of flux. It is found that the oxidizability of steel has significant effect on dephosphoriztion when using the BaO-CaO-CaF2 flux. The phosphate capacity of the used system varied from 1018 to 1019.35 in 1 813-1 893 K and increased with the increasing of BaO content.

Key concepts: Flux (metallurgy), Phosphorus, Materials science, Metallurgy, Liquid steel, Phosphate, Chemistry, Mineralogy