Control Measures to Reduce Slab Triangle Crack Ratio in Iron and Steel Company

Han Peiji

Open publisher page 0 citations

Abstract

Aimed at the cracks of continuous casting slab in the triangle area in early production of an Iron and Steel Co.,the formation mechanism of the cracks of continuous casting slab in the triangle area was studied,the effects of secondary cooling,chemical composition of the steel grade,casting machine condition,the process operation and other factors on the crack formation were analyzed,the measures to prevent the crack in triangular area from generation were put forward.In actual production,the ideas and methods how to quickly analyze and determine the cause of the crack,and to use symptomatic measures were introduced.

About this research paper

What this paper is about

Aimed at the cracks of continuous casting slab in the triangle area in early production of an Iron and Steel Co.,the formation mechanism of the cracks of continuous casting slab in the triangle area was studied,the effects of secondary cooling,chemical composition of the steel grade,casting machine condition,the process operation and other factors on the crack formation were analyzed,the measures to prevent the crack in triangular area from generation were put forward.In actual production,the ideas and methods how to quickly analyze and determine the cause of the crack,and to use symptomatic measures were introduced.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Aimed at the cracks of continuous casting slab in the triangle area in early production of an Iron and Steel Co.,the formation mechanism of the cracks of continuous casting slab in the triangle area was studied,the effects of secondary cooling,chemical composition of the steel grade,casting machine condition,the process operation and other factors on the crack formation were analyzed,the measures to prevent the crack in triangular area from generation were put forward.In actual production,the ideas and methods how to quickly analyze and determine the cause of the crack,and to use symptomatic measures were introduced.

Key concepts: Slab, Continuous casting, Casting, Metallurgy, Steel company, Materials science, Structural engineering, Fracture (geology)

Related papers

Back to paper searchBrowse research topicsOriginal source
Control Measures to Reduce Slab Triangle Crack Ratio in Iron and Steel Company — Research Paper | ScholarLens