Preparation of Fine Nickel Oxide Powder
Liu Song
Abstract
Liu Song
Abstract
The fine nickel oxide powder with the particle size 1~5 μm has been prepared by the oxalate precipitation_calcination method with nickel sulfate as material. The optimal process conditions have been proposed: c (NiSO 4)=0.5~1.5 mol/L, n (C 2O 2- 4)∶ n (Ni 2+ )=1.2~1.3∶1, pH=4~5, precipitation temperature is 45~55 ℃, calcination temperature 500~900 ℃, calcination time 4~6 h.
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
The fine nickel oxide powder with the particle size 1~5 μm has been prepared by the oxalate precipitation_calcination method with nickel sulfate as material. The optimal process conditions have been proposed: c (NiSO 4)=0.5~1.5 mol/L, n (C 2O 2- 4)∶ n (Ni 2+ )=1.2~1.3∶1, pH=4~5, precipitation temperature is 45~55 ℃, calcination temperature 500~900 ℃, calcination time 4~6 h.