In this paper, to find out the best technological conditions of extracting microcrystalline cellulose from corncob by using high pressure cooking method. The optimum concentration of NaOH of the extraction of microcrystalline cellulose is 50% with the method of high pressure cooking. Preparation of carboxymethyl cellulose (CMC) from microcrystalline cellulose was carried out by an etherification process, using NaOH and monochloroacetic acid (MCA), with ethanol and water as the supporting medium. The results indicated that the best reaction condition was that the microcrystalline cellulose were alkalizated at 30 °C for 50 min and etherificated at 65 °C for 3 h, 85% ethanol as solvent with the molar ratio of cellulose/NaOH/MCA was 1:1:1. NaOH is added in three batches with total amount the ratio is 6:2.5:1.5. Under the optimized reaction conditions, the substitution degree (DS) of CMC is 1.02 and the viscosity is 6 mPa's, which possessed special characteristics of low viscosity.
OpenAlex reports 75 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
In this paper, to find out the best technological conditions of extracting microcrystalline cellulose from corncob by using high pressure cooking method. The optimum concentration of NaOH of the extraction of microcrystalline cellulose is 50% with the method of high pressure cooking. Preparation of carboxymethyl cellulose (CMC) from microcrystalline cellulose was carried out by an etherification process, using NaOH and monochloroacetic acid (MCA), with ethanol and water as the supporting medium. The results indicated that the best reaction condition was that the microcrystalline cellulose were alkalizated at 30 °C for 50 min and etherificated at 65 °C for 3 h, 85% ethanol as solvent with the molar ratio of cellulose/NaOH/MCA was 1:1:1. NaOH is added in three batches with total amount the ratio is 6:2.5:1.5. Under the optimized reaction conditions, the substitution degree (DS) of CMC is 1.02 and the viscosity is 6 mPa's, which possessed special characteristics of low viscosity.
Key concepts: Microcrystalline cellulose, Corncob, Carboxymethyl cellulose, Cellulose, Chemistry, Ethanol, Microcrystalline, Solvent