An isolated native mesophilic iron-oxidizing bacteria, acidithiobacillus ferrooxidans, was used to extract zinc by the bioleaching method from a typical lead-zinc tailing. Experiments were carried out by mixed culture of the mesophilic strain in the shake flasks and the different influencing factors such as pH, temperature, inoculation cell number, as well as slurry concentration on the process of bioleaching were investigated. The results indicated that the extraction efficiency of zinc was relevant with these variables and more than 70% of sphalerite was dissolved on the condition of with pH 2.0, initial ferrous concentration of 10 g/L and slurry concentration of 10 wt.% during 25 d, while without bacteria, 22% of Zn was merely extracted.
OpenAlex reports 10 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
An isolated native mesophilic iron-oxidizing bacteria, acidithiobacillus ferrooxidans, was used to extract zinc by the bioleaching method from a typical lead-zinc tailing. Experiments were carried out by mixed culture of the mesophilic strain in the shake flasks and the different influencing factors such as pH, temperature, inoculation cell number, as well as slurry concentration on the process of bioleaching were investigated. The results indicated that the extraction efficiency of zinc was relevant with these variables and more than 70% of sphalerite was dissolved on the condition of with pH 2.0, initial ferrous concentration of 10 g/L and slurry concentration of 10 wt.% during 25 d, while without bacteria, 22% of Zn was merely extracted.
Key concepts: Bioleaching, Mesophile, Sphalerite, Ferrous, Zinc, Chemistry, Oxidizing agent, Slurry