Two types of patterns were tested for castability: 1) polyester mesh pattern (20mm x 22mm with 100 open squares) and 2) 20mm x 20mm wax plates 1.0 and 1.5 mm in thickness. These materials were invested using a pre-arranged commercial phosphate-bonded investment for titanium. Three different types of casting machines were selected: 1) a pressure-type casting machine with separate melting and casting chambers, 2) a pressure-type casting machine with one chamber and 3) a centrifugal-type casting machine at 3000 rpm. Pure titanium (> 99.5%) was cast into the molds at a mold temperature of 100 degrees C. The castability of mesh pattern was evaluated in terms of the number of cast segment, and the cast plate was evaluated using X-ray transparent images by a digital imaging technique. The centrifugal casting method showed the best castability among these three casting methods.
OpenAlex reports 38 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
Two types of patterns were tested for castability: 1) polyester mesh pattern (20mm x 22mm with 100 open squares) and 2) 20mm x 20mm wax plates 1.0 and 1.5 mm in thickness. These materials were invested using a pre-arranged commercial phosphate-bonded investment for titanium. Three different types of casting machines were selected: 1) a pressure-type casting machine with separate melting and casting chambers, 2) a pressure-type casting machine with one chamber and 3) a centrifugal-type casting machine at 3000 rpm. Pure titanium (> 99.5%) was cast into the molds at a mold temperature of 100 degrees C. The castability of mesh pattern was evaluated in terms of the number of cast segment, and the cast plate was evaluated using X-ray transparent images by a digital imaging technique. The centrifugal casting method showed the best castability among these three casting methods.
Key concepts: Castability, Materials science, Casting, Titanium, Centrifugal casting (silversmithing), Metallurgy, Investment casting, Mold