Preparation of Hard Metal Bonded with Fe-Al Alloy.

Keizo Kobayashi, Kenji Miwa, Minoru Fukunaga, Masahiro N. Machida

Open full text 14 citations

Abstract

WC-8.6mass%Fe-1.4mass%Al and WC-6.7mass%Fe-3.3mass%Al alloys were prepared by sintering of wet-mixed powder of WC, Fe and AI at 1713K for 2.4ksec in a vacuum and then their hot isostatic pressing.The evaporation of 13% Al from WC-Fe-Al alloys have been observed in the fabricating process. The sintered WC-Fe-Al alloys have a fine microstructure. Especially, the WC-8.6mass%Fe-1.4mass%AI alloy, which has a few pores after sintering at 1713K, has 1.8GPa of TRS and 92.5HRA of hardness. Furthermore, the increase in weight due to oxidation in this alloy is about one half that of the conventional WC-12mass%Co alloy.

Open-access reader

About this research paper

What this paper is about

WC-8.6mass%Fe-1.4mass%Al and WC-6.7mass%Fe-3.3mass%Al alloys were prepared by sintering of wet-mixed powder of WC, Fe and AI at 1713K for 2.4ksec in a vacuum and then their hot isostatic pressing.The evaporation of 13% Al from WC-Fe-Al alloys have been observed in the fabricating process. The sintered WC-Fe-Al alloys have a fine microstructure. Especially, the WC-8.6mass%Fe-1.4mass%AI alloy, which has a few pores after sintering at 1713K, has 1.8GPa of TRS and 92.5HRA of hardness. Furthermore, the increase in weight due to oxidation in this alloy is about one half that of the conventional WC-12mass%Co alloy.

Why it matters

OpenAlex reports 14 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

WC-8.6mass%Fe-1.4mass%Al and WC-6.7mass%Fe-3.3mass%Al alloys were prepared by sintering of wet-mixed powder of WC, Fe and AI at 1713K for 2.4ksec in a vacuum and then their hot isostatic pressing.The evaporation of 13% Al from WC-Fe-Al alloys have been observed in the fabricating process. The sintered WC-Fe-Al alloys have a fine microstructure. Especially, the WC-8.6mass%Fe-1.4mass%AI alloy, which has a few pores after sintering at 1713K, has 1.8GPa of TRS and 92.5HRA of hardness. Furthermore, the increase in weight due to oxidation in this alloy is about one half that of the conventional WC-12mass%Co alloy.

Key concepts: Alloy, Materials science, Sintering, Metallurgy, Microstructure, Hot isostatic pressing, Hard metal, Pressing

Related papers

Back to paper searchBrowse research topicsOriginal source
Preparation of Hard Metal Bonded with Fe-Al Alloy. — Research Paper | ScholarLens