Mechanical Properties of SiC Whisker-Reinforced TiB2 Composites Fabricated by Hot-Pressing
Akira Kamiya, Kikuo Nakano
Abstract
Open-access reader
Akira Kamiya, Kikuo Nakano
Abstract
Open-access reader
SiC whisker reinforced TiB2 matrix composites containing 10 to 30vol% whisker were prepared by hotpressing at 1600 to 1900°C. The flexural strength of 867±77MPa and KIC of 5.8±0.12MPa√m were obtained for the 1800°C hot-pressed samples containing 10vol% whisker. No significant increase in KIC was observed by the whisker reinforcement because of the chemical reaction between matrix and whisker, which enhanced strong interfacial bonding and whisker agglomeration.
OpenAlex reports 4 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
SiC whisker reinforced TiB2 matrix composites containing 10 to 30vol% whisker were prepared by hotpressing at 1600 to 1900°C. The flexural strength of 867±77MPa and KIC of 5.8±0.12MPa√m were obtained for the 1800°C hot-pressed samples containing 10vol% whisker. No significant increase in KIC was observed by the whisker reinforcement because of the chemical reaction between matrix and whisker, which enhanced strong interfacial bonding and whisker agglomeration.
Key concepts: Whisker, Materials science, Composite material, Hot pressing, Flexural strength, Reinforcement, Monocrystalline whisker, Pressing