Mechanical Properties of Boron-Doped CVD Diamond Films
Sadao Takeuchi, Takashi MURAISHI
Abstract
Open-access reader
Sadao Takeuchi, Takashi MURAISHI
Abstract
Open-access reader
For this study, single-crystal and polycrystalline diamond films with different boron contents were synthesized in a hot-filament chemical vapor deposition (CVD) apparatus to evaluate the mechanical properties of these films. Boron was added to the diamond by introducing B(CH3)3 :trimethyl boron diluted to 1000 ppm with hydrogen into the diamond-synthesis atmosphere. The synthesized diamond film's crystallinity was evaluated using Raman spectroscopy. The Hertz fracture strength was measured using a diamond-ball indenter. Furthermore, the wear resistance of the film was evaluated using a wear testing machine.The results indicate that the crystallinity of the single-crystal diamond film increased concomitantly with increasing boron content. Furthermore, the Hertz fracture strength increased by 20% with the addition of boron. Results clarified that the wear volume of polycrystalline diamond film decreased to approximately one-third its usual value by the addition of boron. These results show that the mechanical properties of boron-doped diamond films can be improved considerably by adding an appropriate amount of boron.
OpenAlex reports 5 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
For this study, single-crystal and polycrystalline diamond films with different boron contents were synthesized in a hot-filament chemical vapor deposition (CVD) apparatus to evaluate the mechanical properties of these films. Boron was added to the diamond by introducing B(CH3)3 :trimethyl boron diluted to 1000 ppm with hydrogen into the diamond-synthesis atmosphere. The synthesized diamond film's crystallinity was evaluated using Raman spectroscopy. The Hertz fracture strength was measured using a diamond-ball indenter. Furthermore, the wear resistance of the film was evaluated using a wear testing machine.The results indicate that the crystallinity of the single-crystal diamond film increased concomitantly with increasing boron content. Furthermore, the Hertz fracture strength increased by 20% with the addition of boron. Results clarified that the wear volume of polycrystalline diamond film decreased to approximately one-third its usual value by the addition of boron. These results show that the mechanical properties of boron-doped diamond films can be improved considerably by adding an appropriate amount of boron.
Key concepts: Diamond, Boron, Materials science, Material properties of diamond, Chemical vapor deposition, Crystallinity, Raman spectroscopy, Composite material