Thermal pretreatment of wood (Lauan) block by torrefaction and its influence on

Wei‐Hsin Chen

Open publisher page 0 citations

Abstract

The purpose of this study is to investigate the torrefaction behavior of woody biomass (Lauan) blocks and its influence on the properties of the wood. Three different torrefaction temperatures of 220, 250 and 280 C, corresponding to light, mild and severe torrefactions, and four torrefaction times of 0.5, 1, 1.5 and 2 h were considered. After analyzing the torrefied woods, it was found that the torrefaction temperature of 280 C was able to increase the calorific value of the wood up to 40%. However, over 50% of weight was lost from the wood. The grindability of the torrefied wood could be improved in a significant way if the torrefaction temperature was as high as 250 C and the torrefaction time longer than 1 h. Therefore, the torrefaction temperature of 250 C along with the torrefaction time longer than 1 h was the recommended operation to intensify the heating value and grindability as well as to avoid too much mass loss of the wood. This study also suggested that over 50% of the reacted wood was converted into condensed liquid. The main components in the liquid were monoaromatics; little amount of heterocyclic hydrocarbons were also obtained from the torrefactions, especially at the torrefaction temperature of 280 C. 2011 Elsevier Ltd. All rights reserved.

About this research paper

What this paper is about

The purpose of this study is to investigate the torrefaction behavior of woody biomass (Lauan) blocks and its influence on the properties of the wood. Three different torrefaction temperatures of 220, 250 and 280 C, corresponding to light, mild and severe torrefactions, and four torrefaction times of 0.5, 1, 1.5 and 2 h were considered. After analyzing the torrefied woods, it was found that the torrefaction temperature of 280 C was able to increase the calorific value of the wood up to 40%. However, over 50% of weight was lost from the wood. The grindability of the torrefied wood could be improved in a significant way if the torrefaction temperature was as high as 250 C and the torrefaction time longer than 1 h. Therefore, the torrefaction temperature of 250 C along with the torrefaction time longer than 1 h was the recommended operation to intensify the heating value and grindability as well as to avoid too much mass loss of the wood. This study also suggested that over 50% of the reacted wood was converted into condensed liquid. The main components in the liquid were monoaromatics; little amount of heterocyclic hydrocarbons were also obtained from the torrefactions, especially at the torrefaction temperature of 280 C. 2011 Elsevier Ltd. All rights reserved.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The purpose of this study is to investigate the torrefaction behavior of woody biomass (Lauan) blocks and its influence on the properties of the wood. Three different torrefaction temperatures of 220, 250 and 280 C, corresponding to light, mild and severe torrefactions, and four torrefaction times of 0.5, 1, 1.5 and 2 h were considered. After analyzing the torrefied woods, it was found that the torrefaction temperature of 280 C was able to increase the calorific value of the wood up to 40%. However, over 50% of weight was lost from the wood. The grindability of the torrefied wood could be improved in a significant way if the torrefaction temperature was as high as 250 C and the torrefaction time longer than 1 h. Therefore, the torrefaction temperature of 250 C along with the torrefaction time longer than 1 h was the recommended operation to intensify the heating value and grindability as well as to avoid too much mass loss of the wood. This study also suggested that over 50% of the reacted wood was converted into condensed liquid. The main components in the liquid were monoaromatics; little amount of heterocyclic hydrocarbons were also obtained from the torrefactions, especially at the torrefaction temperature of 280 C. 2011 Elsevier Ltd. All rights reserved.

Key concepts: Torrefaction, Pulp and paper industry, Heat of combustion, Biomass (ecology), Materials science, Waste management, Chemistry, Pyrolysis