Hydration of the combinations of ground granulated blast furnace slag cements

Noor Azline Mohd Nasir, Farah Nora Aznieta Abdul Aziz, Nor Azizi Safiee

Open publisher page 9 citations

Abstract

Article history: The heat of hydration is known as a measurement of the initial chemical reactions for the hydration of cement. The heat liberated during the hydration process affects the temperature rise in concrete, which may cause an early-age thermal cracking of a concrete structure. To address this thermal cracking issue, Portland cement/ground granulated blast furnace slag (PC/GGBS) is often used, due to the low heat hydration properties of GGBS. This paper presents the results of isothermal conduction calorimetry tests performed on GGBS binary cement, Portland cement/ground granulated blast furnace slag (PC/GGBS), GGBS ternary cement, and Portland cement/ground granulated blast furnace slag/metakaolin (PC/GGBS/MK). The tests covered a range of GGBS levels, which are up to 75% GGBS level and up to 15% MK content by mass for the ternary cement combinations. For PC/GGBS cement, the total heat of hydration is lower than that of PC, and an increase in the GGBS levels resulted in a decrease in the amount of heat liberated; however, for PC/GGBS/MK, the heat of hydration generated is lower than that of PC but is greater than those of the equivalent PC/GGBS, which has an equivalent PC content.

About this research paper

What this paper is about

Article history: The heat of hydration is known as a measurement of the initial chemical reactions for the hydration of cement. The heat liberated during the hydration process affects the temperature rise in concrete, which may cause an early-age thermal cracking of a concrete structure. To address this thermal cracking issue, Portland cement/ground granulated blast furnace slag (PC/GGBS) is often used, due to the low heat hydration properties of GGBS. This paper presents the results of isothermal conduction calorimetry tests performed on GGBS binary cement, Portland cement/ground granulated blast furnace slag (PC/GGBS), GGBS ternary cement, and Portland cement/ground granulated blast furnace slag/metakaolin (PC/GGBS/MK). The tests covered a range of GGBS levels, which are up to 75% GGBS level and up to 15% MK content by mass for the ternary cement combinations. For PC/GGBS cement, the total heat of hydration is lower than that of PC, and an increase in the GGBS levels resulted in a decrease in the amount of heat liberated; however, for PC/GGBS/MK, the heat of hydration generated is lower than that of PC but is greater than those of the equivalent PC/GGBS, which has an equivalent PC content.

Why it matters

OpenAlex reports 9 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Article history: The heat of hydration is known as a measurement of the initial chemical reactions for the hydration of cement. The heat liberated during the hydration process affects the temperature rise in concrete, which may cause an early-age thermal cracking of a concrete structure. To address this thermal cracking issue, Portland cement/ground granulated blast furnace slag (PC/GGBS) is often used, due to the low heat hydration properties of GGBS. This paper presents the results of isothermal conduction calorimetry tests performed on GGBS binary cement, Portland cement/ground granulated blast furnace slag (PC/GGBS), GGBS ternary cement, and Portland cement/ground granulated blast furnace slag/metakaolin (PC/GGBS/MK). The tests covered a range of GGBS levels, which are up to 75% GGBS level and up to 15% MK content by mass for the ternary cement combinations. For PC/GGBS cement, the total heat of hydration is lower than that of PC, and an increase in the GGBS levels resulted in a decrease in the amount of heat liberated; however, for PC/GGBS/MK, the heat of hydration generated is lower than that of PC but is greater than those of the equivalent PC/GGBS, which has an equivalent PC content.

Key concepts: Ground granulated blast-furnace slag, Cement, Portland cement, Materials science, Slag (welding), Metallurgy, Cracking, Composite material