2004Clay MineralsRequires access

Long-term in vitro transformation of 2-line ferrihydrite to goethite/hematite at 4, 10, 15 and 25°C

U. Schwertmann, Helge Stanjek, H. H. Becher

Open publisher page 207 citations

Abstract

Abstract 2-line ferrihydrite stored in water at ambient temperatures from 4 to 25°C and at ten different pH values between 2.5 and 12 for up to 10–12 y transformed to both goethite and hematite at all temperatures and pH values except at pH 12 where only goethite was formed. The rate and degree of transformation (20–100%) increased with increasing pH and temperature. The hematite/ (hematite+goethite) ratio varied between 0 and ~0.8, increased with increasing temperature and showed a strong maximum at pH 7–8 which increased from 0.1–0.2 at 4°C to 0.7–0.8 at 25°C. The maximum coincides with the zero point of charge of ferrihydrite where its solubility and, thus, its via-solution transformation rate to goethite are minimal. We assume, therefore, that in this pH-range the (slower) via-solution transformation to hematite can more efficiently compete with that to goethite.

About this research paper

What this paper is about

Abstract 2-line ferrihydrite stored in water at ambient temperatures from 4 to 25°C and at ten different pH values between 2.5 and 12 for up to 10–12 y transformed to both goethite and hematite at all temperatures and pH values except at pH 12 where only goethite was formed. The rate and degree of transformation (20–100%) increased with increasing pH and temperature. The hematite/ (hematite+goethite) ratio varied between 0 and ~0.8, increased with increasing temperature and showed a strong maximum at pH 7–8 which increased from 0.1–0.2 at 4°C to 0.7–0.8 at 25°C. The maximum coincides with the zero point of charge of ferrihydrite where its solubility and, thus, its via-solution transformation rate to goethite are minimal. We assume, therefore, that in this pH-range the (slower) via-solution transformation to hematite can more efficiently compete with that to goethite.

Why it matters

OpenAlex reports 207 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Abstract 2-line ferrihydrite stored in water at ambient temperatures from 4 to 25°C and at ten different pH values between 2.5 and 12 for up to 10–12 y transformed to both goethite and hematite at all temperatures and pH values except at pH 12 where only goethite was formed. The rate and degree of transformation (20–100%) increased with increasing pH and temperature. The hematite/ (hematite+goethite) ratio varied between 0 and ~0.8, increased with increasing temperature and showed a strong maximum at pH 7–8 which increased from 0.1–0.2 at 4°C to 0.7–0.8 at 25°C. The maximum coincides with the zero point of charge of ferrihydrite where its solubility and, thus, its via-solution transformation rate to goethite are minimal. We assume, therefore, that in this pH-range the (slower) via-solution transformation to hematite can more efficiently compete with that to goethite.

Key concepts: Goethite, Hematite, Ferrihydrite, Solubility, Chemistry, Inorganic chemistry, Mineralogy, Physical chemistry

Related papers

Back to paper searchBrowse research topicsOriginal source
Long-term in vitro transformation of 2-line ferrihydrite to goethite/hematite at 4, 10, 15 and 25°C — Research Paper | ScholarLens