We have obtained zinc oxide (ZnO) in the form of nanocrystallites with crystallite sizes from 46 nm to 3 nm by milling 1.4 micron ZnO powders in the high energy ball mill (HEBM) for the different times: 1, 5 and 8 hours. Crystal structure changes of the ZnO nanocrystallites were studied by x-ray diffraction techniquies. It was established appearance of two new phases: pure zinc (Zn) and cubic zinc oxide (ZnO) among the initial hexagonal zinc oxide phase. From the x-ray patterns by using Scherrer equation have been determined nanocrystallite sizes of samples with the different milling times. Also, by using PCCS with Nanophox we have found particle diameters, their distributions and specific surface area values for each sample. By using Rietveld method are calculated crystal lattice parameters of the hexagonal ZnO, the main phase.

About this research paper

What this paper is about

We have obtained zinc oxide (ZnO) in the form of nanocrystallites with crystallite sizes from 46 nm to 3 nm by milling 1.4 micron ZnO powders in the high energy ball mill (HEBM) for the different times: 1, 5 and 8 hours. Crystal structure changes of the ZnO nanocrystallites were studied by x-ray diffraction techniquies. It was established appearance of two new phases: pure zinc (Zn) and cubic zinc oxide (ZnO) among the initial hexagonal zinc oxide phase. From the x-ray patterns by using Scherrer equation have been determined nanocrystallite sizes of samples with the different milling times. Also, by using PCCS with Nanophox we have found particle diameters, their distributions and specific surface area values for each sample. By using Rietveld method are calculated crystal lattice parameters of the hexagonal ZnO, the main phase.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

We have obtained zinc oxide (ZnO) in the form of nanocrystallites with crystallite sizes from 46 nm to 3 nm by milling 1.4 micron ZnO powders in the high energy ball mill (HEBM) for the different times: 1, 5 and 8 hours. Crystal structure changes of the ZnO nanocrystallites were studied by x-ray diffraction techniquies. It was established appearance of two new phases: pure zinc (Zn) and cubic zinc oxide (ZnO) among the initial hexagonal zinc oxide phase. From the x-ray patterns by using Scherrer equation have been determined nanocrystallite sizes of samples with the different milling times. Also, by using PCCS with Nanophox we have found particle diameters, their distributions and specific surface area values for each sample. By using Rietveld method are calculated crystal lattice parameters of the hexagonal ZnO, the main phase.

Key concepts: Nanocrystalline material, Ball mill, Crystallite, Materials science, Zinc, Scherrer equation, Rietveld refinement, Hexagonal phase

Related papers

Back to paper searchBrowse research topicsOriginal source
Nanocrystalline ZnO powder prepared by high energy ball mill — Research Paper | ScholarLens