The Balance of Titanium and Vanadium in the Blast Furnace with the Use of Sinter Containing a Titanium-Vanadium-Magnetite Concentrate
R. Budzik
Abstract
R. Budzik
Abstract
The investigation concerned the use of sinter containing a titanium-vanadium-magnetite concentrate for the production of pig iron. Sinter containing 0,46 to 0,51 % TiO2 and 0,056 to 0,060 % vanadium was used for pig iron production in the blast furnace. Introducing 200 kg of this concentrate to the1 Mg sinter mix did not cause any deterioration of sinter quality.
OpenAlex reports 6 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
The investigation concerned the use of sinter containing a titanium-vanadium-magnetite concentrate for the production of pig iron. Sinter containing 0,46 to 0,51 % TiO2 and 0,056 to 0,060 % vanadium was used for pig iron production in the blast furnace. Introducing 200 kg of this concentrate to the1 Mg sinter mix did not cause any deterioration of sinter quality.
Key concepts: Vanadium, Titanium, Magnetite, Materials science, Metallurgy, Blast furnace