Cure kinetics of aqueous phenol–formaldehyde resins used for oriented strandboard manufacturing: Analytical technique

Yong Lei, Qinglin Wu, Kun Lian

Open publisher page 47 citations

Abstract

Abstract The cure kinetics of commercial phenol–formaldehyde (PF), used as oriented strandboard face and core resins, were studied using isothermal and dynamic differential scanning calorimetry (DSC). The cure of the face resin completely followed an nth‐order reaction mechanism. The reaction order was nearly 1 with activation energy of 79.29 kJ mol−1. The core resin showed a more complicated cure mechanism, including both nth‐order and autocatalytic reactions. The nth‐order part, with reaction order of 2.38, began at lower temperatures, but the reaction rate of the autocatalytic part increased much faster with increase in curing temperature. The total reaction order for the autocatalytic part was about 5. Cure kinetic models, for both face and core resins, were developed. It is shown that the models fitted experimental data well, and that the isothermal DSC was much more reliable than the dynamic DSC in studying the cure kinetics. Furthermore, the relationships among cure reaction conversion (curing degree), cure temperature, and cure time were predicted for both resin systems. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 100: 1642–1650, 2006

About this research paper

What this paper is about

Abstract The cure kinetics of commercial phenol–formaldehyde (PF), used as oriented strandboard face and core resins, were studied using isothermal and dynamic differential scanning calorimetry (DSC). The cure of the face resin completely followed an nth‐order reaction mechanism. The reaction order was nearly 1 with activation energy of 79.29 kJ mol−1. The core resin showed a more complicated cure mechanism, including both nth‐order and autocatalytic reactions. The nth‐order part, with reaction order of 2.38, began at lower temperatures, but the reaction rate of the autocatalytic part increased much faster with increase in curing temperature. The total reaction order for the autocatalytic part was about 5. Cure kinetic models, for both face and core resins, were developed. It is shown that the models fitted experimental data well, and that the isothermal DSC was much more reliable than the dynamic DSC in studying the cure kinetics. Furthermore, the relationships among cure reaction conversion (curing degree), cure temperature, and cure time were predicted for both resin systems. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 100: 1642–1650, 2006

Why it matters

OpenAlex reports 47 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Abstract The cure kinetics of commercial phenol–formaldehyde (PF), used as oriented strandboard face and core resins, were studied using isothermal and dynamic differential scanning calorimetry (DSC). The cure of the face resin completely followed an nth‐order reaction mechanism. The reaction order was nearly 1 with activation energy of 79.29 kJ mol−1. The core resin showed a more complicated cure mechanism, including both nth‐order and autocatalytic reactions. The nth‐order part, with reaction order of 2.38, began at lower temperatures, but the reaction rate of the autocatalytic part increased much faster with increase in curing temperature. The total reaction order for the autocatalytic part was about 5. Cure kinetic models, for both face and core resins, were developed. It is shown that the models fitted experimental data well, and that the isothermal DSC was much more reliable than the dynamic DSC in studying the cure kinetics. Furthermore, the relationships among cure reaction conversion (curing degree), cure temperature, and cure time were predicted for both resin systems. © 2006 Wiley Periodicals, Inc. J Appl Polym Sci 100: 1642–1650, 2006

Key concepts: Autocatalysis, Curing (chemistry), Differential scanning calorimetry, Order of reaction, Materials science, Activation energy, Kinetics, Isothermal process