Abstract

Crystalline silicon surface passivation by amorphous silicon deposited by three different chemical vapor deposition (CVD) techniques at low (T∼130 °C) temperatures is compared. For all three techniques, surface recombination velocities (SRVs) are reduced by two orders of magnitude after prolonged thermal annealing at 200 °C. This reduction correlates with a decreased dangling bond density at the amorphous-crystalline interface, indicating that dangling bond saturation is the predominant mechanism. All three deposition methods yield excellent surface passivation. For a-Si:H layers deposited by radio frequency plasma enhanced CVD, we obtain outstanding carrier lifetimes of 10.3 ms, corresponding to SRVs below 1.32 cm/s.

Open-access reader

About this research paper

What this paper is about

Crystalline silicon surface passivation by amorphous silicon deposited by three different chemical vapor deposition (CVD) techniques at low (T∼130 °C) temperatures is compared. For all three techniques, surface recombination velocities (SRVs) are reduced by two orders of magnitude after prolonged thermal annealing at 200 °C. This reduction correlates with a decreased dangling bond density at the amorphous-crystalline interface, indicating that dangling bond saturation is the predominant mechanism. All three deposition methods yield excellent surface passivation. For a-Si:H layers deposited by radio frequency plasma enhanced CVD, we obtain outstanding carrier lifetimes of 10.3 ms, corresponding to SRVs below 1.32 cm/s.

Why it matters

OpenAlex reports 64 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Crystalline silicon surface passivation by amorphous silicon deposited by three different chemical vapor deposition (CVD) techniques at low (T∼130 °C) temperatures is compared. For all three techniques, surface recombination velocities (SRVs) are reduced by two orders of magnitude after prolonged thermal annealing at 200 °C. This reduction correlates with a decreased dangling bond density at the amorphous-crystalline interface, indicating that dangling bond saturation is the predominant mechanism. All three deposition methods yield excellent surface passivation. For a-Si:H layers deposited by radio frequency plasma enhanced CVD, we obtain outstanding carrier lifetimes of 10.3 ms, corresponding to SRVs below 1.32 cm/s.

Key concepts: Dangling bond, Passivation, Materials science, Chemical vapor deposition, Amorphous silicon, Silicon, Crystalline silicon, Plasma-enhanced chemical vapor deposition

Related papers

Back to paper searchBrowse research topicsOriginal source
Excellent crystalline silicon surface passivation by amorphous silicon irrespective of the technique used for chemical vapor deposition — Research Paper | ScholarLens