2013Journal of Prosthodontic ResearchOpen access

Effect of loading conditions on the fracture toughness of zirconia

Kosuke Harada, Akikazu Shinya, Akikazu Shinya, Daiichiro Yokoyama, Akiyoshi Shinya, Akiyoshi Shinya

Open full text 57 citations

Abstract

PURPOSE: A Vickers hardness indenter was pressed into yttria-stabilized zirconia (Y-TZP) by the indentation fracture method (IF method). METHODS: The effect on the calculated Vickers hardness, fracture toughness values, and indentation fracture load (9.8, 49, 98, 196, and 294 N) was examined to deduce the optimum conditions of the IF method. Calculated Vickers hardness and fracture toughness values were analyzed with one-way analysis of variance and then multiple comparisons (Scheffe). The appearance of on indentation and cracks was also evaluated using a scanning electron microscopy (SEM). RESULTS: Indentation of Y-TZP was generated by 9.8 and 49 N of indentation fracture load, however cracks could not be confirmed with the microscope attached to the Vickers hardness tester. Both indentation and cracks were observed at 98, 196 and 294 N of indentation fracture load obtained values of 7.1 and 6.8 MPam(1/2). Cracks noted at the 98 N were not clear, whereas the 196 and 294 N showed especially clear cracks. Due to the hardness of zirconia and the light loads, fracture toughness values for 9.8, 49, and 98 N could not be calculated. There was no significant difference between 196 and 294 N, when calculated fracture toughness values were analyzed with multiple comparisons. SEM revealed clear indentation and cracks, that extended linearly, but no chips or fractures were observed. Surface changes were observed at 196 and 294 N that are presumed to be accompanied by phase transition around the cracks. CONCLUSIONS: Optimum experimental conditions of the indentation fracture load in the IF method were determined as 196 and 294 N.

About this research paper

What this paper is about

PURPOSE: A Vickers hardness indenter was pressed into yttria-stabilized zirconia (Y-TZP) by the indentation fracture method (IF method). METHODS: The effect on the calculated Vickers hardness, fracture toughness values, and indentation fracture load (9.8, 49, 98, 196, and 294 N) was examined to deduce the optimum conditions of the IF method. Calculated Vickers hardness and fracture toughness values were analyzed with one-way analysis of variance and then multiple comparisons (Scheffe). The appearance of on indentation and cracks was also evaluated using a scanning electron microscopy (SEM). RESULTS: Indentation of Y-TZP was generated by 9.8 and 49 N of indentation fracture load, however cracks could not be confirmed with the microscope attached to the Vickers hardness tester. Both indentation and cracks were observed at 98, 196 and 294 N of indentation fracture load obtained values of 7.1 and 6.8 MPam(1/2). Cracks noted at the 98 N were not clear, whereas the 196 and 294 N showed especially clear cracks. Due to the hardness of zirconia and the light loads, fracture toughness values for 9.8, 49, and 98 N could not be calculated. There was no significant difference between 196 and 294 N, when calculated fracture toughness values were analyzed with multiple comparisons. SEM revealed clear indentation and cracks, that extended linearly, but no chips or fractures were observed. Surface changes were observed at 196 and 294 N that are presumed to be accompanied by phase transition around the cracks. CONCLUSIONS: Optimum experimental conditions of the indentation fracture load in the IF method were determined as 196 and 294 N.

Why it matters

OpenAlex reports 57 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

PURPOSE: A Vickers hardness indenter was pressed into yttria-stabilized zirconia (Y-TZP) by the indentation fracture method (IF method). METHODS: The effect on the calculated Vickers hardness, fracture toughness values, and indentation fracture load (9.8, 49, 98, 196, and 294 N) was examined to deduce the optimum conditions of the IF method. Calculated Vickers hardness and fracture toughness values were analyzed with one-way analysis of variance and then multiple comparisons (Scheffe). The appearance of on indentation and cracks was also evaluated using a scanning electron microscopy (SEM). RESULTS: Indentation of Y-TZP was generated by 9.8 and 49 N of indentation fracture load, however cracks could not be confirmed with the microscope attached to the Vickers hardness tester. Both indentation and cracks were observed at 98, 196 and 294 N of indentation fracture load obtained values of 7.1 and 6.8 MPam(1/2). Cracks noted at the 98 N were not clear, whereas the 196 and 294 N showed especially clear cracks. Due to the hardness of zirconia and the light loads, fracture toughness values for 9.8, 49, and 98 N could not be calculated. There was no significant difference between 196 and 294 N, when calculated fracture toughness values were analyzed with multiple comparisons. SEM revealed clear indentation and cracks, that extended linearly, but no chips or fractures were observed. Surface changes were observed at 196 and 294 N that are presumed to be accompanied by phase transition around the cracks. CONCLUSIONS: Optimum experimental conditions of the indentation fracture load in the IF method were determined as 196 and 294 N.

Key concepts: Indentation, Fracture toughness, Materials science, Composite material, Vickers hardness test, Cubic zirconia, Scanning electron microscope, Indentation hardness