Chitosan Nanoparticles for siRNA Delivery: Optimization of Processing/Formulation Parameters

Elina Esmaeilzadeh Gharehdaghi, Amir Amani, Mohammad Reza Khoshayand, Mehdi Banan, Elika Esmaeilzadeh Gharehdaghi, Mohammad Ali Amini, Mohammad Ali Faramarzi

Open full text 12 citations

Abstract

Chitosan nanoparticles were prepared using ultrasonication methodology at specific amplitudes and times of sonication. Subsequently, small interfering RNA (siRNA) was added to the solution at predetermined values of nitrogen to phosphorous ratio (N/P), and stirring time. Employing response surfaces generated from a statistical model, the effect of sonication time and amplitude, stirring time, and N/P ratio was studied on the particle size, polydispersity, and loading efficiency of prepared siRNA/chitosan nanoparticles. It was found that to obtain the smallest size, amplitude and time of sonication as well as stirring time should be kept at ∼45%, 165 seconds, and 50 minutes, respectively. Minimum polydispersity values were also obtained at similar values of sonication time/amplitude and stirring time in addition to N/P values of ∼28. Also, the maximum proportion of siRNA loading was observed at approximate values of 300 seconds, 80% and 280 for sonication time, amplitude, and N/P ratio, respectively. The optimum conditions (i.e., to prepare a sample with minimum values of particle size and polydispersity index and maximum values of loading efficiency) were determined as 60.6, 30.0 (seconds), 28.0, and 12.5 (minutes) for amplitude, time of sonication, N/P, and stirring time, respectively. In this scrutiny, the predicted values of optimum formulation were 456 nm size, 89.6% loading efficiency, and 0.4 polydispersity index.

About this research paper

What this paper is about

Chitosan nanoparticles were prepared using ultrasonication methodology at specific amplitudes and times of sonication. Subsequently, small interfering RNA (siRNA) was added to the solution at predetermined values of nitrogen to phosphorous ratio (N/P), and stirring time. Employing response surfaces generated from a statistical model, the effect of sonication time and amplitude, stirring time, and N/P ratio was studied on the particle size, polydispersity, and loading efficiency of prepared siRNA/chitosan nanoparticles. It was found that to obtain the smallest size, amplitude and time of sonication as well as stirring time should be kept at ∼45%, 165 seconds, and 50 minutes, respectively. Minimum polydispersity values were also obtained at similar values of sonication time/amplitude and stirring time in addition to N/P values of ∼28. Also, the maximum proportion of siRNA loading was observed at approximate values of 300 seconds, 80% and 280 for sonication time, amplitude, and N/P ratio, respectively. The optimum conditions (i.e., to prepare a sample with minimum values of particle size and polydispersity index and maximum values of loading efficiency) were determined as 60.6, 30.0 (seconds), 28.0, and 12.5 (minutes) for amplitude, time of sonication, N/P, and stirring time, respectively. In this scrutiny, the predicted values of optimum formulation were 456 nm size, 89.6% loading efficiency, and 0.4 polydispersity index.

Why it matters

OpenAlex reports 12 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Chitosan nanoparticles were prepared using ultrasonication methodology at specific amplitudes and times of sonication. Subsequently, small interfering RNA (siRNA) was added to the solution at predetermined values of nitrogen to phosphorous ratio (N/P), and stirring time. Employing response surfaces generated from a statistical model, the effect of sonication time and amplitude, stirring time, and N/P ratio was studied on the particle size, polydispersity, and loading efficiency of prepared siRNA/chitosan nanoparticles. It was found that to obtain the smallest size, amplitude and time of sonication as well as stirring time should be kept at ∼45%, 165 seconds, and 50 minutes, respectively. Minimum polydispersity values were also obtained at similar values of sonication time/amplitude and stirring time in addition to N/P values of ∼28. Also, the maximum proportion of siRNA loading was observed at approximate values of 300 seconds, 80% and 280 for sonication time, amplitude, and N/P ratio, respectively. The optimum conditions (i.e., to prepare a sample with minimum values of particle size and polydispersity index and maximum values of loading efficiency) were determined as 60.6, 30.0 (seconds), 28.0, and 12.5 (minutes) for amplitude, time of sonication, N/P, and stirring time, respectively. In this scrutiny, the predicted values of optimum formulation were 456 nm size, 89.6% loading efficiency, and 0.4 polydispersity index.

Key concepts: Sonication, Dispersity, Chitosan, Particle size, Materials science, Nanoparticle, Analytical Chemistry (journal), Particle (ecology)