2010Polymers for Advanced TechnologiesRequires access

Morphology and properties of natural rubber with nanomatrix of non‐rubber components

Seiichi Kawahara, Oraphin Chaikumpollert, Keiichi Akabori, Yoshimasa Yamamoto

Open publisher page 53 citations

Abstract

Abstract The morphology of natural rubber was observed by transmission electron microscopy. Nanomatrix of non‐rubber components such as proteins and phospholipids was found to be inherently formed in natural rubber, in which natural rubber particles of about 0.5 µm in average diameter were dispersed. The nanomatrix of non‐rubber components disappeared after deproteinization of natural rubber with urea. Stress at break of serum rubber was higher than that of deproteinized natural rubber, while strain at break did not change. When the amount of the non‐rubber components increased, the stress at break became significantly dependent upon the amount of non‐rubber components. Viscoelastic properties of natural rubber were also dependent upon the nanomatrix of non‐rubber components. Storage modulus of natural rubber increased significantly, when the amount of the non‐rubber components increased. Copyright © 2010 John Wiley & Sons, Ltd.

About this research paper

What this paper is about

Abstract The morphology of natural rubber was observed by transmission electron microscopy. Nanomatrix of non‐rubber components such as proteins and phospholipids was found to be inherently formed in natural rubber, in which natural rubber particles of about 0.5 µm in average diameter were dispersed. The nanomatrix of non‐rubber components disappeared after deproteinization of natural rubber with urea. Stress at break of serum rubber was higher than that of deproteinized natural rubber, while strain at break did not change. When the amount of the non‐rubber components increased, the stress at break became significantly dependent upon the amount of non‐rubber components. Viscoelastic properties of natural rubber were also dependent upon the nanomatrix of non‐rubber components. Storage modulus of natural rubber increased significantly, when the amount of the non‐rubber components increased. Copyright © 2010 John Wiley & Sons, Ltd.

Why it matters

OpenAlex reports 53 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Abstract The morphology of natural rubber was observed by transmission electron microscopy. Nanomatrix of non‐rubber components such as proteins and phospholipids was found to be inherently formed in natural rubber, in which natural rubber particles of about 0.5 µm in average diameter were dispersed. The nanomatrix of non‐rubber components disappeared after deproteinization of natural rubber with urea. Stress at break of serum rubber was higher than that of deproteinized natural rubber, while strain at break did not change. When the amount of the non‐rubber components increased, the stress at break became significantly dependent upon the amount of non‐rubber components. Viscoelastic properties of natural rubber were also dependent upon the nanomatrix of non‐rubber components. Storage modulus of natural rubber increased significantly, when the amount of the non‐rubber components increased. Copyright © 2010 John Wiley & Sons, Ltd.

Key concepts: Natural rubber, Materials science, Composite material, Dynamic mechanical analysis, Synthetic rubber, Modulus, Viscoelasticity, Morphology (biology)

Related papers

Back to paper searchBrowse research topicsOriginal source
Morphology and properties of natural rubber with nanomatrix of non‐rubber components — Research Paper | ScholarLens