Abstract

Iron-carbon micro-electrolysis was applied in the treatment of the electroplating wastewater containing copper, and the parameters that affected the efficiencies of the wastewater treatment had been discussed, The results indicated that the optimal experimental conditions were initial pH 4, stirring speed 100r/min, total mass of iron and carbon 4g/0.1L, iron carbon mass ratio of 1, reaction time was 40min. The removal rate of the Cu2+was 99% or more, the effluent can meet emissions standards

About this research paper

What this paper is about

Iron-carbon micro-electrolysis was applied in the treatment of the electroplating wastewater containing copper, and the parameters that affected the efficiencies of the wastewater treatment had been discussed, The results indicated that the optimal experimental conditions were initial pH 4, stirring speed 100r/min, total mass of iron and carbon 4g/0.1L, iron carbon mass ratio of 1, reaction time was 40min. The removal rate of the Cu2+was 99% or more, the effluent can meet emissions standards

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Iron-carbon micro-electrolysis was applied in the treatment of the electroplating wastewater containing copper, and the parameters that affected the efficiencies of the wastewater treatment had been discussed, The results indicated that the optimal experimental conditions were initial pH 4, stirring speed 100r/min, total mass of iron and carbon 4g/0.1L, iron carbon mass ratio of 1, reaction time was 40min. The removal rate of the Cu2+was 99% or more, the effluent can meet emissions standards

Key concepts: Electrolysis, Wastewater, Electroplating, Effluent, Copper, Carbon fibers, Metallurgy, Materials science

Related papers

Back to paper searchBrowse research topicsOriginal source
Research on Micro-Electrolysis Method to Treat the Copper-Containing Electroplating Wastewater — Research Paper | ScholarLens