2013Applied Mechanics and MaterialsOpen access

Recovery of Copper from Flotation Tailings by Leaching

Dan Liu, Shu Ming Wen, Yong Jun Xian, Hai Ying Shen, Jiushuai Deng, Dan Dan Wu

Open full text 1 citations

Abstract

A technology route of Reverse flotation of acid-consuming gangue mineralsAcid leaching for copperExtractingElectrodepositing is proposed for recovery copper from a tailings with high content of calcium oxide and magnesium oxide and high content of combined copper oxide. The effect of H2SO4 concentration, leaching time and stirring speed on copper leaching was investigated. The leaching solution obtained under the optimal copper leaching conditions, was used to be proceeded for extracting and electrodepositing test. The best leaching conditions are stirring speed of 30 m/min, H2SO4 concentration of 150 Kg/t ore, leaching time of 30 minutes. Under the best conditions, the acid leaching test presented that the production of per ton copper consumes sulfuric acid of 17.31 t, and Cu leaching rate is 84.70%.

About this research paper

What this paper is about

A technology route of Reverse flotation of acid-consuming gangue mineralsAcid leaching for copperExtractingElectrodepositing is proposed for recovery copper from a tailings with high content of calcium oxide and magnesium oxide and high content of combined copper oxide. The effect of H2SO4 concentration, leaching time and stirring speed on copper leaching was investigated. The leaching solution obtained under the optimal copper leaching conditions, was used to be proceeded for extracting and electrodepositing test. The best leaching conditions are stirring speed of 30 m/min, H2SO4 concentration of 150 Kg/t ore, leaching time of 30 minutes. Under the best conditions, the acid leaching test presented that the production of per ton copper consumes sulfuric acid of 17.31 t, and Cu leaching rate is 84.70%.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

A technology route of Reverse flotation of acid-consuming gangue mineralsAcid leaching for copperExtractingElectrodepositing is proposed for recovery copper from a tailings with high content of calcium oxide and magnesium oxide and high content of combined copper oxide. The effect of H2SO4 concentration, leaching time and stirring speed on copper leaching was investigated. The leaching solution obtained under the optimal copper leaching conditions, was used to be proceeded for extracting and electrodepositing test. The best leaching conditions are stirring speed of 30 m/min, H2SO4 concentration of 150 Kg/t ore, leaching time of 30 minutes. Under the best conditions, the acid leaching test presented that the production of per ton copper consumes sulfuric acid of 17.31 t, and Cu leaching rate is 84.70%.

Key concepts: Leaching (pedology), Tailings, Gangue, Copper, Sulfuric acid, Copper extraction techniques, Metallurgy, Magnesium