2004Materials science forumOpen access

Preparation and Characterization of Organic Light Emitting Devices Using QD Dopant

Jung Yohn Cho, Ho Chang

Open full text 2 citations

Abstract

Two types of the organic light-emitting devices (OLEDs) with different emission structures were prepared using Alq3 (aluminum tris 8-hydroxyquinoline) host material and quinacridone (QD) dopant at the emission layer. One is the OLED device with emission layer consisting of Alq3 host material doped with QD dopant ("codoped OLED"). The another one has a seperated QD dopant film in the Alq3 emission layer ("undoped OLED"). The maximum brightness of the codoped and undoped OLEDs were 3207 cd/m2 and 1570 cd/m2, respectively. The wavelength of the maximum emission peak in the undoped sample was 527 nm and shifted slightly toward longer wavelength with the value of 540 nm for the codoped OLED sample. The maximum luminous efficiency of the undoped OLED was about 1.4 lm/W and increased to 7.0 lm/W for the codoped sample.

About this research paper

What this paper is about

Two types of the organic light-emitting devices (OLEDs) with different emission structures were prepared using Alq3 (aluminum tris 8-hydroxyquinoline) host material and quinacridone (QD) dopant at the emission layer. One is the OLED device with emission layer consisting of Alq3 host material doped with QD dopant ("codoped OLED"). The another one has a seperated QD dopant film in the Alq3 emission layer ("undoped OLED"). The maximum brightness of the codoped and undoped OLEDs were 3207 cd/m2 and 1570 cd/m2, respectively. The wavelength of the maximum emission peak in the undoped sample was 527 nm and shifted slightly toward longer wavelength with the value of 540 nm for the codoped OLED sample. The maximum luminous efficiency of the undoped OLED was about 1.4 lm/W and increased to 7.0 lm/W for the codoped sample.

Why it matters

OpenAlex reports 2 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Two types of the organic light-emitting devices (OLEDs) with different emission structures were prepared using Alq3 (aluminum tris 8-hydroxyquinoline) host material and quinacridone (QD) dopant at the emission layer. One is the OLED device with emission layer consisting of Alq3 host material doped with QD dopant ("codoped OLED"). The another one has a seperated QD dopant film in the Alq3 emission layer ("undoped OLED"). The maximum brightness of the codoped and undoped OLEDs were 3207 cd/m2 and 1570 cd/m2, respectively. The wavelength of the maximum emission peak in the undoped sample was 527 nm and shifted slightly toward longer wavelength with the value of 540 nm for the codoped OLED sample. The maximum luminous efficiency of the undoped OLED was about 1.4 lm/W and increased to 7.0 lm/W for the codoped sample.

Key concepts: OLED, Dopant, Materials science, Optoelectronics, Doping, Layer (electronics), Brightness, Optics

Related papers

Back to paper searchBrowse research topicsOriginal source
Preparation and Characterization of Organic Light Emitting Devices Using QD Dopant — Research Paper | ScholarLens