Abstract

The atrazine-degrading bacterial strain Pseudomonas sp. ADP was immobilized by the sol–gel process within thin silica layers coated onto water-retaining carrier materials (expanded clay pellets and scoria). The performance of the obtained biohybrid material has been investigated concerning long-term activity under non-growth conditions. Experiments were run in phosphate buffer containing atrazine (20 mg l−1) as the sole source of carbon and nitrogen. Even after one year of consecutive batch tests, P. ADP immobilized onto expanded clay pellets showed a high atrazine degradation activity. In the course of long-term batch experiments, the average amount of removed atrazine was about 94% during each assay cycle. Staining with CTC revealed that in spite of cultivation under non-growth conditions over a period of one year, immobilized cells were still vital and showed respiratory activity.

Open-access reader

About this research paper

What this paper is about

The atrazine-degrading bacterial strain Pseudomonas sp. ADP was immobilized by the sol–gel process within thin silica layers coated onto water-retaining carrier materials (expanded clay pellets and scoria). The performance of the obtained biohybrid material has been investigated concerning long-term activity under non-growth conditions. Experiments were run in phosphate buffer containing atrazine (20 mg l−1) as the sole source of carbon and nitrogen. Even after one year of consecutive batch tests, P. ADP immobilized onto expanded clay pellets showed a high atrazine degradation activity. In the course of long-term batch experiments, the average amount of removed atrazine was about 94% during each assay cycle. Staining with CTC revealed that in spite of cultivation under non-growth conditions over a period of one year, immobilized cells were still vital and showed respiratory activity.

Why it matters

OpenAlex reports 9 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The atrazine-degrading bacterial strain Pseudomonas sp. ADP was immobilized by the sol–gel process within thin silica layers coated onto water-retaining carrier materials (expanded clay pellets and scoria). The performance of the obtained biohybrid material has been investigated concerning long-term activity under non-growth conditions. Experiments were run in phosphate buffer containing atrazine (20 mg l−1) as the sole source of carbon and nitrogen. Even after one year of consecutive batch tests, P. ADP immobilized onto expanded clay pellets showed a high atrazine degradation activity. In the course of long-term batch experiments, the average amount of removed atrazine was about 94% during each assay cycle. Staining with CTC revealed that in spite of cultivation under non-growth conditions over a period of one year, immobilized cells were still vital and showed respiratory activity.

Key concepts: Atrazine, Pseudomonas, Chemistry, Bacteria, Microbiology, Chromatography, Food science, Nuclear chemistry

Related papers

Back to paper searchBrowse research topicsOriginal source
Long-term activity of biohybrid coatings of atrazine-degrading bacteria Pseudomonas sp. ADP — Research Paper | ScholarLens