2002Journal of Materials Processing TechnologyOpen access

Stress corrosion cracking susceptibility of Al–Mg alloy sheet with high Mg content

Miljana Popović, Endre Romhanji

Open full text 75 citations

Abstract

Slow strain rate testing (SSRT) was used to study the effect of the microstructure on the stress corrosion cracking (SCC) susceptibility of Al–Mg alloy sheet containing 6.8 wt.% Mg. In the cold-rolled and fully annealed conditions, high SCC susceptibility was experienced. In those cases the ductility was strongly affected by the presence of corrosive environment (for hard temper: Elair=13.6%, ElSCC=0.6%; for annealed condition: Elair=24.1–25.3%, ElSCC=3.2–4.2%) and the elongation loss was great, Elloss=81.7–95.6%. It is supposed that the high SCC susceptibility results from a continuous network of the β-phase (Mg5Al8) precipitate at grain boundaries for the annealed temper, and heavy precipitation of β-phase along the planes of localized deformation for the hard temper. High SCC resistance attained after thermal exposure at the temperature range 225–285 °C (stabilized condition). The ductility was almost unaffected by the presence of corrosive environment (Elair=12.8–23.2%, ElSCC=12.8–22%) and the elongation loss was small, Elloss<7%. High SCC resistance was related to the stabilized structure, which causes discontinuous β-phase (Mg5Al8) precipitation in a globular form, uniformly distributed throughout the structure.

About this research paper

What this paper is about

Slow strain rate testing (SSRT) was used to study the effect of the microstructure on the stress corrosion cracking (SCC) susceptibility of Al–Mg alloy sheet containing 6.8 wt.% Mg. In the cold-rolled and fully annealed conditions, high SCC susceptibility was experienced. In those cases the ductility was strongly affected by the presence of corrosive environment (for hard temper: Elair=13.6%, ElSCC=0.6%; for annealed condition: Elair=24.1–25.3%, ElSCC=3.2–4.2%) and the elongation loss was great, Elloss=81.7–95.6%. It is supposed that the high SCC susceptibility results from a continuous network of the β-phase (Mg5Al8) precipitate at grain boundaries for the annealed temper, and heavy precipitation of β-phase along the planes of localized deformation for the hard temper. High SCC resistance attained after thermal exposure at the temperature range 225–285 °C (stabilized condition). The ductility was almost unaffected by the presence of corrosive environment (Elair=12.8–23.2%, ElSCC=12.8–22%) and the elongation loss was small, Elloss<7%. High SCC resistance was related to the stabilized structure, which causes discontinuous β-phase (Mg5Al8) precipitation in a globular form, uniformly distributed throughout the structure.

Why it matters

OpenAlex reports 75 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Slow strain rate testing (SSRT) was used to study the effect of the microstructure on the stress corrosion cracking (SCC) susceptibility of Al–Mg alloy sheet containing 6.8 wt.% Mg. In the cold-rolled and fully annealed conditions, high SCC susceptibility was experienced. In those cases the ductility was strongly affected by the presence of corrosive environment (for hard temper: Elair=13.6%, ElSCC=0.6%; for annealed condition: Elair=24.1–25.3%, ElSCC=3.2–4.2%) and the elongation loss was great, Elloss=81.7–95.6%. It is supposed that the high SCC susceptibility results from a continuous network of the β-phase (Mg5Al8) precipitate at grain boundaries for the annealed temper, and heavy precipitation of β-phase along the planes of localized deformation for the hard temper. High SCC resistance attained after thermal exposure at the temperature range 225–285 °C (stabilized condition). The ductility was almost unaffected by the presence of corrosive environment (Elair=12.8–23.2%, ElSCC=12.8–22%) and the elongation loss was small, Elloss<7%. High SCC resistance was related to the stabilized structure, which causes discontinuous β-phase (Mg5Al8) precipitation in a globular form, uniformly distributed throughout the structure.

Key concepts: Materials science, Stress corrosion cracking, Metallurgy, Alloy, Microstructure, Elongation, Ductility (Earth science), Corrosion

Related papers

Back to paper searchBrowse research topicsOriginal source
Stress corrosion cracking susceptibility of Al–Mg alloy sheet with high Mg content — Research Paper | ScholarLens