2010Advanced materials researchOpen access

Comparing Age Hardening Behaviors of Al-3Cu and Al-8Si-3Cu Alloys

Gui Qing Wang, Yan Liu, Guo Cheng Ren, Zhong Kui Zhao

Open full text 1 citations

Abstract

The aging hardening behaviors of Al-8Si-3%Cu (wt%) and Al-3Cu (wt%) alloys have been investigated. Samples were solution treated at 500 for 24 h followed by water quenching before aging. Hardness has been measured for quenched samples aging at 150°C. Strong age hardening occurs for Al-3Cu alloy and hardness increases by about 60% after peak aging. There is a hardness decrease in the early aging stage of Al-8Si-3Cu alloy and hardness increases by about 15% after peak aging. The age precipitation behaviors have been analyzed using DSC and TEM. Effects of microstructure characteristics on age precipitation and age hardening response of Al-8Si-3Cu alloy have been discussed.

About this research paper

What this paper is about

The aging hardening behaviors of Al-8Si-3%Cu (wt%) and Al-3Cu (wt%) alloys have been investigated. Samples were solution treated at 500 for 24 h followed by water quenching before aging. Hardness has been measured for quenched samples aging at 150°C. Strong age hardening occurs for Al-3Cu alloy and hardness increases by about 60% after peak aging. There is a hardness decrease in the early aging stage of Al-8Si-3Cu alloy and hardness increases by about 15% after peak aging. The age precipitation behaviors have been analyzed using DSC and TEM. Effects of microstructure characteristics on age precipitation and age hardening response of Al-8Si-3Cu alloy have been discussed.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The aging hardening behaviors of Al-8Si-3%Cu (wt%) and Al-3Cu (wt%) alloys have been investigated. Samples were solution treated at 500 for 24 h followed by water quenching before aging. Hardness has been measured for quenched samples aging at 150°C. Strong age hardening occurs for Al-3Cu alloy and hardness increases by about 60% after peak aging. There is a hardness decrease in the early aging stage of Al-8Si-3Cu alloy and hardness increases by about 15% after peak aging. The age precipitation behaviors have been analyzed using DSC and TEM. Effects of microstructure characteristics on age precipitation and age hardening response of Al-8Si-3Cu alloy have been discussed.

Key concepts: Precipitation hardening, Alloy, Hardening (computing), Materials science, Microstructure, Precipitation, Metallurgy, Quenching (fluorescence)