1999Journal of Laser ApplicationsRequires access

Study on prevention of welding defects in high power CO2 laser materials processing

Toshifumi Matsumoto, Naoaki Fukuda, Yasuo Kondo, Akira Ohmori, Katsunori Inoue, Yoshiaki Arata

Open publisher page 2 citations

Abstract

For CO2 laser welding of large output, when a deep penetration welding in single pass is done in the ambient atmosphere, it is known that blowholes may occur because of the in-keyhole gas being entrapped in molten metal. Keeping this problem in mind and changing the parameters, we conducted welding tests with full-penetration bead-on-plate welding, and checked by radiographic test for welding defects. The experimental results demonstrated that the larger the specimen thickness, the more frequently welding defects occur, and that generation of welding defects depends upon the amount of welding heat input. Welding defects such as blowholes remain in metal, because the gas once entrapped into keyhole floats up in molten metal, and it is enclosed in the course of solidification. From this, we can verify the theory that a larger welding heat input, in the case of the good appearance full-penetration bead-on-plate welding, may be favorable for preventing welding blowholes. It can be assumed, therefore, that a larger heat input may hinder cooling of molten metal, and need a longer time for metal solidification; in this longer span of time, in-molten metal gas may escape while the metal is sufficiently heated.

About this research paper

What this paper is about

For CO2 laser welding of large output, when a deep penetration welding in single pass is done in the ambient atmosphere, it is known that blowholes may occur because of the in-keyhole gas being entrapped in molten metal. Keeping this problem in mind and changing the parameters, we conducted welding tests with full-penetration bead-on-plate welding, and checked by radiographic test for welding defects. The experimental results demonstrated that the larger the specimen thickness, the more frequently welding defects occur, and that generation of welding defects depends upon the amount of welding heat input. Welding defects such as blowholes remain in metal, because the gas once entrapped into keyhole floats up in molten metal, and it is enclosed in the course of solidification. From this, we can verify the theory that a larger welding heat input, in the case of the good appearance full-penetration bead-on-plate welding, may be favorable for preventing welding blowholes. It can be assumed, therefore, that a larger heat input may hinder cooling of molten metal, and need a longer time for metal solidification; in this longer span of time, in-molten metal gas may escape while the metal is sufficiently heated.

Why it matters

OpenAlex reports 2 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

For CO2 laser welding of large output, when a deep penetration welding in single pass is done in the ambient atmosphere, it is known that blowholes may occur because of the in-keyhole gas being entrapped in molten metal. Keeping this problem in mind and changing the parameters, we conducted welding tests with full-penetration bead-on-plate welding, and checked by radiographic test for welding defects. The experimental results demonstrated that the larger the specimen thickness, the more frequently welding defects occur, and that generation of welding defects depends upon the amount of welding heat input. Welding defects such as blowholes remain in metal, because the gas once entrapped into keyhole floats up in molten metal, and it is enclosed in the course of solidification. From this, we can verify the theory that a larger welding heat input, in the case of the good appearance full-penetration bead-on-plate welding, may be favorable for preventing welding blowholes. It can be assumed, therefore, that a larger heat input may hinder cooling of molten metal, and need a longer time for metal solidification; in this longer span of time, in-molten metal gas may escape while the metal is sufficiently heated.

Key concepts: Welding, Materials science, Laser beam welding, Heat-affected zone, Electric resistance welding, Keyhole, Metallurgy, Gas metal arc welding

Related papers

Back to paper searchBrowse research topicsOriginal source
Study on prevention of welding defects in high power CO2 laser materials processing — Research Paper | ScholarLens