The Influence of the Milling Environment on the Structure of a W-Cu Composite
Franciné A. Costa, Francisco Ambrózio Filho, A.G.P. Silva, Uílame Umbelino Gomes, Severino Jackson Guedes de Lima, Wilson Acchar
Abstract
Franciné A. Costa, Francisco Ambrózio Filho, A.G.P. Silva, Uílame Umbelino Gomes, Severino Jackson Guedes de Lima, Wilson Acchar
Abstract
This work reports an investigation about the influence of the environment of milling on the characteristics of the powders and on the structure and density of sintered samples made of these powders. Mixtures of composition W-30wt%Cu were milled for 51 hours in a high energy planetary mill in dry and wet (cyclohexane) conditions. The milled powders have composite particles. The powders were pressed and sintered at 1050º, 1150º and 1200°C under flowing hydrogen. The isothermal times were 0 minutes for the first two temperatures and 60 minutes for the latter. The samples reached around 95% of relative density. The powders were characterized by means of XRD and SEM. The sintered samples were characterized by means of SEM, optical microscopy and density measurement.
A significance statement is not available in the OpenAlex record.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
This work reports an investigation about the influence of the environment of milling on the characteristics of the powders and on the structure and density of sintered samples made of these powders. Mixtures of composition W-30wt%Cu were milled for 51 hours in a high energy planetary mill in dry and wet (cyclohexane) conditions. The milled powders have composite particles. The powders were pressed and sintered at 1050º, 1150º and 1200°C under flowing hydrogen. The isothermal times were 0 minutes for the first two temperatures and 60 minutes for the latter. The samples reached around 95% of relative density. The powders were characterized by means of XRD and SEM. The sintered samples were characterized by means of SEM, optical microscopy and density measurement.
Key concepts: Materials science, Isothermal process, Composite number, Cyclohexane, Relative density, Optical microscope, Wet-milling, Composite material