The interaction of thin (<1 nm) samarium films deposited on a textured iridium ribbon has been investigated by thermal desorption spectrometry. Samarium atoms deposited at T = 300 K desorb in three phases associated with the formation of a submonolayer samarium coverage on iridium, a compound of samarium with iridium, and a multilayer samarium film. The interaction with oxygen leads to the appearance of a new desorption phase, which is associated with the formation of samarium oxide. Oxidation of samarium is observed during exposure in oxygen already at room temperature. An increase in temperature of the iridium ribbon, at which exposure in oxygen occurs, to T = 1100 K leads to the formation of the compound of samarium with iridium. Further, the film of the compound decomposes in the course of interaction with oxygen, and samarium oxide grows on the Ir surface.

About this research paper

What this paper is about

The interaction of thin (<1 nm) samarium films deposited on a textured iridium ribbon has been investigated by thermal desorption spectrometry. Samarium atoms deposited at T = 300 K desorb in three phases associated with the formation of a submonolayer samarium coverage on iridium, a compound of samarium with iridium, and a multilayer samarium film. The interaction with oxygen leads to the appearance of a new desorption phase, which is associated with the formation of samarium oxide. Oxidation of samarium is observed during exposure in oxygen already at room temperature. An increase in temperature of the iridium ribbon, at which exposure in oxygen occurs, to T = 1100 K leads to the formation of the compound of samarium with iridium. Further, the film of the compound decomposes in the course of interaction with oxygen, and samarium oxide grows on the Ir surface.

Why it matters

OpenAlex reports 6 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The interaction of thin (<1 nm) samarium films deposited on a textured iridium ribbon has been investigated by thermal desorption spectrometry. Samarium atoms deposited at T = 300 K desorb in three phases associated with the formation of a submonolayer samarium coverage on iridium, a compound of samarium with iridium, and a multilayer samarium film. The interaction with oxygen leads to the appearance of a new desorption phase, which is associated with the formation of samarium oxide. Oxidation of samarium is observed during exposure in oxygen already at room temperature. An increase in temperature of the iridium ribbon, at which exposure in oxygen occurs, to T = 1100 K leads to the formation of the compound of samarium with iridium. Further, the film of the compound decomposes in the course of interaction with oxygen, and samarium oxide grows on the Ir surface.

Key concepts: Samarium, Iridium, Materials science, Oxygen, Desorption, Thermal desorption, Oxide, Inorganic chemistry

Related papers

Back to paper searchBrowse research topicsOriginal source
Initial stages of the interaction with oxygen of samarium thin films grown on the iridium surface — Research Paper | ScholarLens