Abstract

The microstructural evolution and elevated temperature tensile properties of Ti-6.6Al-5.2Sn-1.8Zr-(0~3.8)Sc (wt%) alloys have been investigated. The Sc-added alloys showed improved yield strength at 650°C and 750°C and with the elongation above 10%. Minor addition of Sc was found to significantly reduce the as-cast grain size. Higher amount of Sc additions resulted in the formation of high density of Sc-oxide, which causes the high strength at elevated temperatures and the reduction of ductility. High density of α2-Ti3Al fine precipitates with an average size of about 20 nm were observed inside equiaxed primary α (αp) grains in the Sc-free or minor Sc added alloys. However, precipitation free zone (PFZ) also formed in those alloys, where grain boundaries are free from any precipitates. Higher Sc addition was found to hinder the formation of PFZ and α2–precipitates.

About this research paper

What this paper is about

The microstructural evolution and elevated temperature tensile properties of Ti-6.6Al-5.2Sn-1.8Zr-(0~3.8)Sc (wt%) alloys have been investigated. The Sc-added alloys showed improved yield strength at 650°C and 750°C and with the elongation above 10%. Minor addition of Sc was found to significantly reduce the as-cast grain size. Higher amount of Sc additions resulted in the formation of high density of Sc-oxide, which causes the high strength at elevated temperatures and the reduction of ductility. High density of α2-Ti3Al fine precipitates with an average size of about 20 nm were observed inside equiaxed primary α (αp) grains in the Sc-free or minor Sc added alloys. However, precipitation free zone (PFZ) also formed in those alloys, where grain boundaries are free from any precipitates. Higher Sc addition was found to hinder the formation of PFZ and α2–precipitates.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The microstructural evolution and elevated temperature tensile properties of Ti-6.6Al-5.2Sn-1.8Zr-(0~3.8)Sc (wt%) alloys have been investigated. The Sc-added alloys showed improved yield strength at 650°C and 750°C and with the elongation above 10%. Minor addition of Sc was found to significantly reduce the as-cast grain size. Higher amount of Sc additions resulted in the formation of high density of Sc-oxide, which causes the high strength at elevated temperatures and the reduction of ductility. High density of α2-Ti3Al fine precipitates with an average size of about 20 nm were observed inside equiaxed primary α (αp) grains in the Sc-free or minor Sc added alloys. However, precipitation free zone (PFZ) also formed in those alloys, where grain boundaries are free from any precipitates. Higher Sc addition was found to hinder the formation of PFZ and α2–precipitates.

Key concepts: Equiaxed crystals, Materials science, Ductility (Earth science), Precipitation, Elongation, Ultimate tensile strength, Metallurgy, Scandium

Related papers

Back to paper searchBrowse research topicsOriginal source
Scandium (Sc) Behavior in High Temperature Ti Alloys — Research Paper | ScholarLens