1999•Journal of The Electrochemical SocietyOpen access

Zinc‐Substituted α‐Nickel Hydroxide as an Electrode Material for Alkaline Secondary Cells

Mridula Dixit, P. Vishnu Kamath, Jagannatha Gopalakrishnan

Open full text 96 citations

Abstract

Double hydroxides of the formula, having the same structure as that of α‐nickel hydroxide have been synthesized by partial substitution of zinc for nickel. The hydroxide having the composition x = 0.25 exhibits prolonged stability in 6 M KOH. Pasted electrodes comprising this material are rechargeable with a stabilized reversible discharge capacity of of nickel even under suboptimal conditions of electrode fabrication. This compares favorably with the capacity values achieved for β‐nickel hydroxide ( , This work; , Delahaye‐Vidal and Figlarz; , theoretical). © 1999 The Electrochemical Society. All rights reserved.

Open-access reader

About this research paper

What this paper is about

Double hydroxides of the formula, having the same structure as that of α‐nickel hydroxide have been synthesized by partial substitution of zinc for nickel. The hydroxide having the composition x = 0.25 exhibits prolonged stability in 6 M KOH. Pasted electrodes comprising this material are rechargeable with a stabilized reversible discharge capacity of of nickel even under suboptimal conditions of electrode fabrication. This compares favorably with the capacity values achieved for β‐nickel hydroxide ( , This work; , Delahaye‐Vidal and Figlarz; , theoretical). © 1999 The Electrochemical Society. All rights reserved.

Why it matters

OpenAlex reports 96 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Double hydroxides of the formula, having the same structure as that of α‐nickel hydroxide have been synthesized by partial substitution of zinc for nickel. The hydroxide having the composition x = 0.25 exhibits prolonged stability in 6 M KOH. Pasted electrodes comprising this material are rechargeable with a stabilized reversible discharge capacity of of nickel even under suboptimal conditions of electrode fabrication. This compares favorably with the capacity values achieved for β‐nickel hydroxide ( , This work; , Delahaye‐Vidal and Figlarz; , theoretical). © 1999 The Electrochemical Society. All rights reserved.

Key concepts: Hydroxide, Nickel, Alkaline battery, Zinc, Electrochemistry, Electrode, Zinc hydroxide, Inorganic chemistry

Related papers

Back to paper searchBrowse research topicsOriginal source
Zinc‐Substituted α‐Nickel Hydroxide as an Electrode Material for Alkaline Secondary Cells — Research Paper | ScholarLens