2013IEICE Transactions on ElectronicsOpen access

Native Oxide Removal from InAlN Surfaces by Hydrofluoric Acid Based Treatment

Takuma Nakano, Masamichi Akazawa

Open full text 2 citations

Abstract

We investigated the effects of chemical treatments for removing native oxide layers on InAlN surfaces by X-ray photoelectron spectroscopy (XPS). The untreated surface of the air exposed InAlN layer was covered with the native oxide layer mainly composed of hydroxides. Hydrochloric acid treatment and ammonium hydroxide treatment were not efficient for removing the native oxide layer even after immersion for 15 min, while hydrofluoric acid (HF) treatment led to a removal in a short treatment time of 1min. After the HF treatment, the surface was prevented from reoxidation in air for 1 h. We also found that the 5-min buffered HF treatment had almost the same effect as the 1-min HF treatment. Finally, an attempt was made to apply the HF-based treatment to the metal-InAlN contact to confirm the XPS results.

Open-access reader

About this research paper

What this paper is about

We investigated the effects of chemical treatments for removing native oxide layers on InAlN surfaces by X-ray photoelectron spectroscopy (XPS). The untreated surface of the air exposed InAlN layer was covered with the native oxide layer mainly composed of hydroxides. Hydrochloric acid treatment and ammonium hydroxide treatment were not efficient for removing the native oxide layer even after immersion for 15 min, while hydrofluoric acid (HF) treatment led to a removal in a short treatment time of 1min. After the HF treatment, the surface was prevented from reoxidation in air for 1 h. We also found that the 5-min buffered HF treatment had almost the same effect as the 1-min HF treatment. Finally, an attempt was made to apply the HF-based treatment to the metal-InAlN contact to confirm the XPS results.

Why it matters

OpenAlex reports 2 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

We investigated the effects of chemical treatments for removing native oxide layers on InAlN surfaces by X-ray photoelectron spectroscopy (XPS). The untreated surface of the air exposed InAlN layer was covered with the native oxide layer mainly composed of hydroxides. Hydrochloric acid treatment and ammonium hydroxide treatment were not efficient for removing the native oxide layer even after immersion for 15 min, while hydrofluoric acid (HF) treatment led to a removal in a short treatment time of 1min. After the HF treatment, the surface was prevented from reoxidation in air for 1 h. We also found that the 5-min buffered HF treatment had almost the same effect as the 1-min HF treatment. Finally, an attempt was made to apply the HF-based treatment to the metal-InAlN contact to confirm the XPS results.

Key concepts: Hydrofluoric acid, X-ray photoelectron spectroscopy, Ammonium hydroxide, Oxide, Hydrochloric acid, Hydroxide, Materials science, Inorganic chemistry

Related papers

Back to paper searchBrowse research topicsOriginal source
Native Oxide Removal from InAlN Surfaces by Hydrofluoric Acid Based Treatment — Research Paper | ScholarLens