2014Advanced materials researchRequires access

The Influences of Additives and Heat Treatment on the Properties of Electroless Plating Ni-W-Mo-P Alloy on the Aluminum

Zu Xiao Yu, De Tao Zheng, Hong Guo, Yong Liu, Yuan Liang Luo, Chao Deng

Open publisher page 0 citations

Abstract

To improve the wear resistance and anti-corrosion properties of the aluminum, the electroless plating Ni-W-Mo-P alloy on the aluminum is necessary. The influences of heat treatment and additives (stabilizers) on the porosity, deposition rate, corrosion current, corrosion potential, microhardness and wear resistance of electroless plating Ni-W-Mo-P alloy coating, were investigated using electrochemical methods, etc. The results show that the deposition rate and anti-corrosion properties of electroless plating Ni-W-Mo-P are improved when the stabilizers, including KI (1mg/L) and “KIO3 (1mg/L) + Pb (Ac)2 (1mg/L)”, are added into bath, respectively. In addition, the maximum hardness (902 HV) and good wear resistance of Ni-W-Mo-P coatings are obtained when heated at 400°C (1h). However, its corrosion resistance is worse. Its microhardness is also obviously improved after heated at 200°Cfor 6 h, and the microhardness reaches to 950 HV.

About this research paper

What this paper is about

To improve the wear resistance and anti-corrosion properties of the aluminum, the electroless plating Ni-W-Mo-P alloy on the aluminum is necessary. The influences of heat treatment and additives (stabilizers) on the porosity, deposition rate, corrosion current, corrosion potential, microhardness and wear resistance of electroless plating Ni-W-Mo-P alloy coating, were investigated using electrochemical methods, etc. The results show that the deposition rate and anti-corrosion properties of electroless plating Ni-W-Mo-P are improved when the stabilizers, including KI (1mg/L) and “KIO3 (1mg/L) + Pb (Ac)2 (1mg/L)”, are added into bath, respectively. In addition, the maximum hardness (902 HV) and good wear resistance of Ni-W-Mo-P coatings are obtained when heated at 400°C (1h). However, its corrosion resistance is worse. Its microhardness is also obviously improved after heated at 200°Cfor 6 h, and the microhardness reaches to 950 HV.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

To improve the wear resistance and anti-corrosion properties of the aluminum, the electroless plating Ni-W-Mo-P alloy on the aluminum is necessary. The influences of heat treatment and additives (stabilizers) on the porosity, deposition rate, corrosion current, corrosion potential, microhardness and wear resistance of electroless plating Ni-W-Mo-P alloy coating, were investigated using electrochemical methods, etc. The results show that the deposition rate and anti-corrosion properties of electroless plating Ni-W-Mo-P are improved when the stabilizers, including KI (1mg/L) and “KIO3 (1mg/L) + Pb (Ac)2 (1mg/L)”, are added into bath, respectively. In addition, the maximum hardness (902 HV) and good wear resistance of Ni-W-Mo-P coatings are obtained when heated at 400°C (1h). However, its corrosion resistance is worse. Its microhardness is also obviously improved after heated at 200°Cfor 6 h, and the microhardness reaches to 950 HV.

Key concepts: Materials science, Indentation hardness, Corrosion, Metallurgy, Alloy, Plating (geology), Aluminium, Coating

Related papers

Back to paper searchBrowse research topicsOriginal source
The Influences of Additives and Heat Treatment on the Properties of Electroless Plating Ni-W-Mo-P Alloy on the Aluminum — Research Paper | ScholarLens