Elemental Chlorine Free (ECF) bleaching sequence of O1/O2D0EOPD1D2 was adopted to bleach the pro-hydrolyzed Larix kraft pulp, where O1/O2 was two-stage oxygen delignification without interstage treatment, D was chlorine dioxide bleaching, EOP was pressurized alkaline extraction strengthened by hydrogen peroxide. Keeping bleaching temperature and time unchanged, sodium hydroxide charge(NaOH) in O1 stage, chlorine dioxide(ClO2) charge in D0 stage and D2 stage were studied, pulp properties such as brightness, kappa number, alpha-cellulose, pentosan and polymerization degree were measured and compared to establish optimal bleaching conditions. Results show that the optimal charge of NaOH in O1 stage is 2.5%, ClO2 in D0 and D2 stage are 2.5%, 0.6%, and the pulp gained at the optimal bleaching conditions has the properties of 93.9% of alpha-cellulose, 2.60% of pentosan, 375.5 ml/g of viscosity and 86.6%ISO of brightness.

About this research paper

What this paper is about

Elemental Chlorine Free (ECF) bleaching sequence of O1/O2D0EOPD1D2 was adopted to bleach the pro-hydrolyzed Larix kraft pulp, where O1/O2 was two-stage oxygen delignification without interstage treatment, D was chlorine dioxide bleaching, EOP was pressurized alkaline extraction strengthened by hydrogen peroxide. Keeping bleaching temperature and time unchanged, sodium hydroxide charge(NaOH) in O1 stage, chlorine dioxide(ClO2) charge in D0 stage and D2 stage were studied, pulp properties such as brightness, kappa number, alpha-cellulose, pentosan and polymerization degree were measured and compared to establish optimal bleaching conditions. Results show that the optimal charge of NaOH in O1 stage is 2.5%, ClO2 in D0 and D2 stage are 2.5%, 0.6%, and the pulp gained at the optimal bleaching conditions has the properties of 93.9% of alpha-cellulose, 2.60% of pentosan, 375.5 ml/g of viscosity and 86.6%ISO of brightness.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Elemental Chlorine Free (ECF) bleaching sequence of O1/O2D0EOPD1D2 was adopted to bleach the pro-hydrolyzed Larix kraft pulp, where O1/O2 was two-stage oxygen delignification without interstage treatment, D was chlorine dioxide bleaching, EOP was pressurized alkaline extraction strengthened by hydrogen peroxide. Keeping bleaching temperature and time unchanged, sodium hydroxide charge(NaOH) in O1 stage, chlorine dioxide(ClO2) charge in D0 stage and D2 stage were studied, pulp properties such as brightness, kappa number, alpha-cellulose, pentosan and polymerization degree were measured and compared to establish optimal bleaching conditions. Results show that the optimal charge of NaOH in O1 stage is 2.5%, ClO2 in D0 and D2 stage are 2.5%, 0.6%, and the pulp gained at the optimal bleaching conditions has the properties of 93.9% of alpha-cellulose, 2.60% of pentosan, 375.5 ml/g of viscosity and 86.6%ISO of brightness.

Key concepts: Chlorine dioxide, Kappa number, Sodium hydroxide, Bleach, Dissolving pulp, Kraft process, Kraft paper, Pulp (tooth)

Related papers

Back to paper searchBrowse research topicsOriginal source
ECF Bleaching of Pre-Hydrolyzed Larix Kraft Pulp for Production of Dissolving Pulp — Research Paper | ScholarLens