2013•Advanced materials researchRequires access

Effects of Oil Palm Empty Fruit Bunch (OPEFB) Fibre Size on Fracture Toughness of OPEFB Filled Polymer Nanocomposite

Rahilah Kamarudzaman, Anizah Kalam, Nurul Natisya Ahmad, Noorrul Wahida Abdul Razak, Z. Salleh

Open publisher page 1 citations

Abstract

The effect of oil palm empty fruit bunch (OPEFB) fiber size on the fracture toughness of OPEFB/PP/PPnanoclay composites was investigated. Four fiber sizes ranging from 180 μm, 250 μm, 300 μm, and 355 μm were used to reinforce PP/PPnanoclay composites. The ratio of PP/PPnanoclay was 7:100 by weight (7 phr). Fracture toughness of the composite was determined according to ASTM D5045 and single edge notch bending (SENB) been employed during the test. The result indicates that the fracture toughness of OPEFB/PP/PPnanoclay composites has decreased as OPEFB fiber size increased. Fracture surfaces investigated through the scanning electron microscopy (SEM) showed that the bonding between fiber and matrix for OPEFB/PP/PPnanoclay composites with smaller OPEFB fibre size has better bonding as compared to OPEFB/PP/PPnanoclay composites with larger OPEFB fiber size.

About this research paper

What this paper is about

The effect of oil palm empty fruit bunch (OPEFB) fiber size on the fracture toughness of OPEFB/PP/PPnanoclay composites was investigated. Four fiber sizes ranging from 180 μm, 250 μm, 300 μm, and 355 μm were used to reinforce PP/PPnanoclay composites. The ratio of PP/PPnanoclay was 7:100 by weight (7 phr). Fracture toughness of the composite was determined according to ASTM D5045 and single edge notch bending (SENB) been employed during the test. The result indicates that the fracture toughness of OPEFB/PP/PPnanoclay composites has decreased as OPEFB fiber size increased. Fracture surfaces investigated through the scanning electron microscopy (SEM) showed that the bonding between fiber and matrix for OPEFB/PP/PPnanoclay composites with smaller OPEFB fibre size has better bonding as compared to OPEFB/PP/PPnanoclay composites with larger OPEFB fiber size.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

The effect of oil palm empty fruit bunch (OPEFB) fiber size on the fracture toughness of OPEFB/PP/PPnanoclay composites was investigated. Four fiber sizes ranging from 180 μm, 250 μm, 300 μm, and 355 μm were used to reinforce PP/PPnanoclay composites. The ratio of PP/PPnanoclay was 7:100 by weight (7 phr). Fracture toughness of the composite was determined according to ASTM D5045 and single edge notch bending (SENB) been employed during the test. The result indicates that the fracture toughness of OPEFB/PP/PPnanoclay composites has decreased as OPEFB fiber size increased. Fracture surfaces investigated through the scanning electron microscopy (SEM) showed that the bonding between fiber and matrix for OPEFB/PP/PPnanoclay composites with smaller OPEFB fibre size has better bonding as compared to OPEFB/PP/PPnanoclay composites with larger OPEFB fiber size.

Key concepts: Materials science, Composite material, Scanning electron microscope, Fiber, Composite number, Fracture toughness, Nanocomposite, Toughness

Related papers

Back to paper searchBrowse research topicsOriginal source
Effects of Oil Palm Empty Fruit Bunch (OPEFB) Fibre Size on Fracture Toughness of OPEFB Filled Polymer Nanocomposite — Research Paper | ScholarLens