2001•LangmuirRequires access

Separation of Adsorbed Formamide and Intercalated Formamide Using Controlled Rate Thermal Analysis Methodology

Ray L. Frost, János Kristóf, Erzsébet Horváth, J. Theo Kloprogge

Open publisher page 24 citations

Abstract

Controlled rate thermal analysis (CRTA) has been used to separate adsorbed formamide from intercalated formamide in formamide-intercalated kaolinites. This separation is achieved by removal of the sample at the end of the controlled isothermal desorption step. The temperature of this isothermal desorption is dependent on the use of open or closed crucibles in the thermal analysis unit but is independent of the formamide/water ratio. X-ray diffraction shows that the formamide-intercalated kaolinite remains expanded after formamide desorption with a d (001) spacing of 10.09 Å. Further heating to 300 °C results in the deintercalation of the formamide-intercalated kaolinite. DRIFT spectroscopy shows differences between the infrared spectra of the adsorbed and formamide-intercalated kaolinites. An intense band observed at 3629 cm - 1 is attributed to the inner surface hydroxyls hydrogen bonded to the formamide. The adsorbed formamide-intercalated kaolinites contain adsorbed water and show intensity in the 1705 cm - 1 band, which is absent in the CRTA-treated formamide-intercalated kaolinites.

About this research paper

What this paper is about

Controlled rate thermal analysis (CRTA) has been used to separate adsorbed formamide from intercalated formamide in formamide-intercalated kaolinites. This separation is achieved by removal of the sample at the end of the controlled isothermal desorption step. The temperature of this isothermal desorption is dependent on the use of open or closed crucibles in the thermal analysis unit but is independent of the formamide/water ratio. X-ray diffraction shows that the formamide-intercalated kaolinite remains expanded after formamide desorption with a d (001) spacing of 10.09 Å. Further heating to 300 °C results in the deintercalation of the formamide-intercalated kaolinite. DRIFT spectroscopy shows differences between the infrared spectra of the adsorbed and formamide-intercalated kaolinites. An intense band observed at 3629 cm - 1 is attributed to the inner surface hydroxyls hydrogen bonded to the formamide. The adsorbed formamide-intercalated kaolinites contain adsorbed water and show intensity in the 1705 cm - 1 band, which is absent in the CRTA-treated formamide-intercalated kaolinites.

Why it matters

OpenAlex reports 24 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Controlled rate thermal analysis (CRTA) has been used to separate adsorbed formamide from intercalated formamide in formamide-intercalated kaolinites. This separation is achieved by removal of the sample at the end of the controlled isothermal desorption step. The temperature of this isothermal desorption is dependent on the use of open or closed crucibles in the thermal analysis unit but is independent of the formamide/water ratio. X-ray diffraction shows that the formamide-intercalated kaolinite remains expanded after formamide desorption with a d (001) spacing of 10.09 Å. Further heating to 300 °C results in the deintercalation of the formamide-intercalated kaolinite. DRIFT spectroscopy shows differences between the infrared spectra of the adsorbed and formamide-intercalated kaolinites. An intense band observed at 3629 cm - 1 is attributed to the inner surface hydroxyls hydrogen bonded to the formamide. The adsorbed formamide-intercalated kaolinites contain adsorbed water and show intensity in the 1705 cm - 1 band, which is absent in the CRTA-treated formamide-intercalated kaolinites.

Key concepts: Formamide, Kaolinite, Adsorption, Chemistry, Desorption, Isothermal process, Thermal desorption, Thermal analysis

Related papers

Back to paper searchBrowse research topicsOriginal source
Separation of Adsorbed Formamide and Intercalated Formamide Using Controlled Rate Thermal Analysis Methodology — Research Paper | ScholarLens