Abstract

SEUMALDI has been successfully used to accurately measure the MW of hydrolysis degradation products from Estane 5703. Reasonable structure assignments have been made to the degradation products and several observations reported. Most of the low MW degradation peaks have been identified as ester hydrolysis fragments. The data suggest that the polyester macrodiol may be shorter than the {approximately}2000 amu reported by the manufacturer. Experiments are ongoing to determine if hydrolysis occurs within the material's applied environment.

Open-access reader

About this research paper

What this paper is about

SEUMALDI has been successfully used to accurately measure the MW of hydrolysis degradation products from Estane 5703. Reasonable structure assignments have been made to the degradation products and several observations reported. Most of the low MW degradation peaks have been identified as ester hydrolysis fragments. The data suggest that the polyester macrodiol may be shorter than the {approximately}2000 amu reported by the manufacturer. Experiments are ongoing to determine if hydrolysis occurs within the material's applied environment.

Why it matters

OpenAlex reports 3 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

SEUMALDI has been successfully used to accurately measure the MW of hydrolysis degradation products from Estane 5703. Reasonable structure assignments have been made to the degradation products and several observations reported. Most of the low MW degradation peaks have been identified as ester hydrolysis fragments. The data suggest that the polyester macrodiol may be shorter than the {approximately}2000 amu reported by the manufacturer. Experiments are ongoing to determine if hydrolysis occurs within the material's applied environment.

Key concepts: Degradation (telecommunications), Hydrolysis, Hydrolytic degradation, Measure (data warehouse), Chemistry, Organic chemistry, Computer science, Data mining