1994Applied Physics LettersRequires access

Defect passivation in multicrystalline-Si materials by plasma-enhanced chemical vapor deposition of SiO2/SiN coatings

Z. Chen, A. Rohatgi, R. O. Bell, J.P. Kalejs

Open publisher page 36 citations

Abstract

It is shown for the first time that plasma-enhanced chemical vapor deposition (PECVD) passivation which involves low temperature PECVD of ∼100 Å SiO2 and ∼600 Å SiN followed by photoassisted anneal is very effective for both surface and bulk defect passivation in multicrystalline-Si materials. It is found that the effective recombination lifetime increased by a factor of 2–10 depending upon the multicrystalline material. Some solar cells were fabricated using a three-layer PECVD coating (100 Å SiO2/600 Å SiN/950 Å SiO2), the bottom two for passivation and the top two for antireflection coating. The bulk and surface passivation effects were quantified and decoupled by a combination of internal quantum efficiency measurements and computer modeling. It was found that the PECVD passivated solar cells increased bulk lifetime from 10 to 20 μs, and decreased the surface recombination velocity from 2×105 to 5×104 cm/s.

About this research paper

What this paper is about

It is shown for the first time that plasma-enhanced chemical vapor deposition (PECVD) passivation which involves low temperature PECVD of ∼100 Å SiO2 and ∼600 Å SiN followed by photoassisted anneal is very effective for both surface and bulk defect passivation in multicrystalline-Si materials. It is found that the effective recombination lifetime increased by a factor of 2–10 depending upon the multicrystalline material. Some solar cells were fabricated using a three-layer PECVD coating (100 Å SiO2/600 Å SiN/950 Å SiO2), the bottom two for passivation and the top two for antireflection coating. The bulk and surface passivation effects were quantified and decoupled by a combination of internal quantum efficiency measurements and computer modeling. It was found that the PECVD passivated solar cells increased bulk lifetime from 10 to 20 μs, and decreased the surface recombination velocity from 2×105 to 5×104 cm/s.

Why it matters

OpenAlex reports 36 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

It is shown for the first time that plasma-enhanced chemical vapor deposition (PECVD) passivation which involves low temperature PECVD of ∼100 Å SiO2 and ∼600 Å SiN followed by photoassisted anneal is very effective for both surface and bulk defect passivation in multicrystalline-Si materials. It is found that the effective recombination lifetime increased by a factor of 2–10 depending upon the multicrystalline material. Some solar cells were fabricated using a three-layer PECVD coating (100 Å SiO2/600 Å SiN/950 Å SiO2), the bottom two for passivation and the top two for antireflection coating. The bulk and surface passivation effects were quantified and decoupled by a combination of internal quantum efficiency measurements and computer modeling. It was found that the PECVD passivated solar cells increased bulk lifetime from 10 to 20 μs, and decreased the surface recombination velocity from 2×105 to 5×104 cm/s.

Key concepts: Passivation, Plasma-enhanced chemical vapor deposition, Materials science, Carrier lifetime, Chemical vapor deposition, Coating, Silicon, Plasma

Related papers

Back to paper searchBrowse research topicsOriginal source
Defect passivation in multicrystalline-Si materials by plasma-enhanced chemical vapor deposition of SiO2/SiN coatings — Research Paper | ScholarLens