BIOACTIVITY OF APATITE–WOLLASTONITE GLASS-CERAMICS PRODUCED BY MELTING CASTING
Jongee Park, Abdullah Öztürk
Abstract
Jongee Park, Abdullah Öztürk
Abstract
Glass-ceramics containing only apatite and wollastonite crystals were produced in the system MgO-CaO-SiO2-P2O5-F by the melt casting process. The bioactivity of the glass-ceramics was determined by immersing the glass-ceramics in a simulated body fluid (SBF) and by assessing the resulting apatite formation on the free surface after various immersion durations. A 12-μm-thick apatite layer formed on the surface of the glass-ceramic containing only apatite crystals after 20 days immersion in SBF. However, the thickness of the apatite layer formed on the surface of the glass-ceramic containing apatite and wollastonite crystals was 1 μm. Results have shown that the bioactivity of glass-ceramic depends strongly on the type of crystal(s) developed during the glass-ceramic process and their proportion in the glassy matrix.
OpenAlex reports 5 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
Glass-ceramics containing only apatite and wollastonite crystals were produced in the system MgO-CaO-SiO2-P2O5-F by the melt casting process. The bioactivity of the glass-ceramics was determined by immersing the glass-ceramics in a simulated body fluid (SBF) and by assessing the resulting apatite formation on the free surface after various immersion durations. A 12-μm-thick apatite layer formed on the surface of the glass-ceramic containing only apatite crystals after 20 days immersion in SBF. However, the thickness of the apatite layer formed on the surface of the glass-ceramic containing apatite and wollastonite crystals was 1 μm. Results have shown that the bioactivity of glass-ceramic depends strongly on the type of crystal(s) developed during the glass-ceramic process and their proportion in the glassy matrix.
Key concepts: Wollastonite, Apatite, Simulated body fluid, Materials science, Ceramic, Glass-ceramic, Composite material, Mineralogy