Localized Corrosion Resistance of Mn-Substituted Austenitic Stainless Steels: Effect of Molybdenum and Chromium
R. J. Brigham, E. W. Tozer
Abstract
R. J. Brigham, E. W. Tozer
Abstract
The pitting and crevice corrosion resistance of a number of Mn-substituted austenitic stainless steels has been determined quantitatively using temperature as a localized corrosion criterion. The go/no-go temperatures, the critical pitting temperature (CPT), and the crevice corrosion temperature (CCT) can be summarized by the equations CPT(C)=22+7×%Mo+5×(%Cr-18)and CCT(C)=-(20±5)+11×%Mo+3.5×(%Cr-18)for Mn-substituted austenitic stainless steels over the composition range 0 to 5% Mo and 18 to 22% Cr. The resistance to localized corrosion of these Cr-Ni-Mn-Mo alloys is compared with that of Cr-Ni-Mo austenitic stainless steels.
OpenAlex reports 22 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
The pitting and crevice corrosion resistance of a number of Mn-substituted austenitic stainless steels has been determined quantitatively using temperature as a localized corrosion criterion. The go/no-go temperatures, the critical pitting temperature (CPT), and the crevice corrosion temperature (CCT) can be summarized by the equations CPT(C)=22+7×%Mo+5×(%Cr-18)and CCT(C)=-(20±5)+11×%Mo+3.5×(%Cr-18)for Mn-substituted austenitic stainless steels over the composition range 0 to 5% Mo and 18 to 22% Cr. The resistance to localized corrosion of these Cr-Ni-Mn-Mo alloys is compared with that of Cr-Ni-Mo austenitic stainless steels.
Key concepts: Metallurgy, Crevice corrosion, Materials science, Austenite, Molybdenum, Corrosion, Chromium, Intergranular corrosion