Fabrication of soft magnetic cores by spark-plasma sintering

S. Yamamoto

Open publisher page 0 citations

Abstract

Nb3Al powder prepared by hydriding–dehydriding was sintered using spark plasma sintering. Experiments on high temperature strength and superconductivity show that the sintered samples have superior properties than those reported elsewhere.

About this research paper

What this paper is about

Nb3Al powder prepared by hydriding–dehydriding was sintered using spark plasma sintering. Experiments on high temperature strength and superconductivity show that the sintered samples have superior properties than those reported elsewhere.

Why it matters

A significance statement is not available in the OpenAlex record.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Nb3Al powder prepared by hydriding–dehydriding was sintered using spark plasma sintering. Experiments on high temperature strength and superconductivity show that the sintered samples have superior properties than those reported elsewhere.

Key concepts: Spark plasma sintering, Materials science, Fabrication, SPARK (programming language), Plasma, Sintering, Composite material, Nanotechnology

Related papers

Back to paper searchBrowse research topicsOriginal source
Fabrication of soft magnetic cores by spark-plasma sintering — Research Paper | ScholarLens