Bacterial leaching kinetics for copper dissolution from a lowgrade Indian chalcopyrite ore
Abhilash, K D Mehta, B D Pandey
Abstract
Open-access reader
Abhilash, K D Mehta, B D Pandey
Abstract
Open-access reader
Bio-leaching of copper (0.3%) from a low grade Indian chalcopyrite ore of Malanjkhand copper mines, using a native mesophilic isolate predominantly Acidithiobacillus ferrooxidans (A.ferrooxidans), is reported. A bio-recovery of 72% Cu was recorded in the presence of this culture (not adapted), which increased to 75% with an ore adapted culture after 35 days at 35ºC and pH 2.0 with <50fim particles. The kinetic data showed best fit for the diffusion-controlled shrinking core model, exhibiting linear plots for [1- 2/3X-(1-X)2/3] vs time (X-fraction leached). Apparently, the role of the bacteria is to convert the ferrous ion to the ferric state, which oxidizes the chalcopyrite in order to dissolve copper, while maintaining a high redox potential. The activation energy value (E) was calculated to be 96 and 108 kJ/mol for the un-adapted culture and the ore adapted culture respectively in the temperature range 25-35ºC. This leaching mechanism was corroborated by XRD phase identification and SEM studies of the leach residue.
OpenAlex reports 18 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
Bio-leaching of copper (0.3%) from a low grade Indian chalcopyrite ore of Malanjkhand copper mines, using a native mesophilic isolate predominantly Acidithiobacillus ferrooxidans (A.ferrooxidans), is reported. A bio-recovery of 72% Cu was recorded in the presence of this culture (not adapted), which increased to 75% with an ore adapted culture after 35 days at 35ºC and pH 2.0 with <50fim particles. The kinetic data showed best fit for the diffusion-controlled shrinking core model, exhibiting linear plots for [1- 2/3X-(1-X)2/3] vs time (X-fraction leached). Apparently, the role of the bacteria is to convert the ferrous ion to the ferric state, which oxidizes the chalcopyrite in order to dissolve copper, while maintaining a high redox potential. The activation energy value (E) was calculated to be 96 and 108 kJ/mol for the un-adapted culture and the ore adapted culture respectively in the temperature range 25-35ºC. This leaching mechanism was corroborated by XRD phase identification and SEM studies of the leach residue.
Key concepts: Chalcopyrite, Copper, Dissolution, Leaching (pedology), Copper extraction techniques, Bioleaching, Ferric, Sulfur