An experimental study on the improvement of particle size distribution of calcite powder (d50 = 3.23 μm) was carried out. Ultrafine grinding of calcite powder was studied under batch wet conditions in a laboratory stirred mill. After grinding, the suspension was allowed to age at 30°C for 12 and 24 h. The results indicated that the fineness narrow particle size distribution is influenced to a small extent by altering some operating parameters, such as suspension temperature and aging time. Further increase in the fineness narrow particle size distribution is likely with additional optimization work on the operating parameters of aging process.

About this research paper

What this paper is about

An experimental study on the improvement of particle size distribution of calcite powder (d50 = 3.23 μm) was carried out. Ultrafine grinding of calcite powder was studied under batch wet conditions in a laboratory stirred mill. After grinding, the suspension was allowed to age at 30°C for 12 and 24 h. The results indicated that the fineness narrow particle size distribution is influenced to a small extent by altering some operating parameters, such as suspension temperature and aging time. Further increase in the fineness narrow particle size distribution is likely with additional optimization work on the operating parameters of aging process.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

An experimental study on the improvement of particle size distribution of calcite powder (d50 = 3.23 μm) was carried out. Ultrafine grinding of calcite powder was studied under batch wet conditions in a laboratory stirred mill. After grinding, the suspension was allowed to age at 30°C for 12 and 24 h. The results indicated that the fineness narrow particle size distribution is influenced to a small extent by altering some operating parameters, such as suspension temperature and aging time. Further increase in the fineness narrow particle size distribution is likely with additional optimization work on the operating parameters of aging process.

Key concepts: Fineness, Grinding, Calcite, Particle-size distribution, Materials science, Particle size, Suspension (topology), Mill

Related papers

Back to paper searchBrowse research topicsOriginal source
Use of Wet Grinding and Aging to Produce Narrow Particle Size Distribution — Research Paper | ScholarLens