Effect of carbon content on hydrogen occlusivity and embrittlement of ferrite–pearlite steels
S.L.I. Chan, J. Andrew Charles
Abstract
S.L.I. Chan, J. Andrew Charles
Abstract
Experiments on a series of pure Fe–C alloys consisting of ferrite and pearlite only have shown that the ferrite/pearlite and pearlite/pearlite interfaces are effective hydrogen trapping sites. The ferrite/cementite interfaces within the pearlite colonies, however, have little effect on the hydrogen occlusivity. With an increase in carbon content, more ferrite/pearlite interfaces are created and these increase the hydrogen occlusivity. Although the ferrite/cementite lamella interface has little effect on the hydrogen occlusivity, it does appear that the lamellae interfere with the hydrogen diffusion path across the pearlite colonies. Thus, the higher-carbon alloys in the pearlitic condition have a lower apparent hydrogen diffusivity. Hydrogen has little effect on the tensile strength, but significantly reduces the ductility. After hydrogen charging, high-carbon alloys suffer a lower ductility loss. However, in terms of absolute values, the low-carbon specimens are always more ductile than the high-carbon alloys when saturated with hydrogen.MST/433
OpenAlex reports 70 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
Experiments on a series of pure Fe–C alloys consisting of ferrite and pearlite only have shown that the ferrite/pearlite and pearlite/pearlite interfaces are effective hydrogen trapping sites. The ferrite/cementite interfaces within the pearlite colonies, however, have little effect on the hydrogen occlusivity. With an increase in carbon content, more ferrite/pearlite interfaces are created and these increase the hydrogen occlusivity. Although the ferrite/cementite lamella interface has little effect on the hydrogen occlusivity, it does appear that the lamellae interfere with the hydrogen diffusion path across the pearlite colonies. Thus, the higher-carbon alloys in the pearlitic condition have a lower apparent hydrogen diffusivity. Hydrogen has little effect on the tensile strength, but significantly reduces the ductility. After hydrogen charging, high-carbon alloys suffer a lower ductility loss. However, in terms of absolute values, the low-carbon specimens are always more ductile than the high-carbon alloys when saturated with hydrogen.MST/433
Key concepts: Pearlite, Cementite, Materials science, Ferrite (magnet), Hydrogen, Hydrogen embrittlement, Metallurgy, Ductility (Earth science)