Silica-clad optical fibers comprising a core of crystalline germanium were drawn using a molten core technique. With respect to previous fibers drawn using a borosilicate cladding, the present fibers exhibit negligible oxygen despite being fabricated at more than twice the melting point of the germanium. The counterintuitive result of less oxygen when the fiber is drawn at a higher temperatures is discussed. The measured propagation loss for the fiber was 0.7 dB/cm at 3.39 μm, which is the lowest loss reported to date.

About this research paper

What this paper is about

Silica-clad optical fibers comprising a core of crystalline germanium were drawn using a molten core technique. With respect to previous fibers drawn using a borosilicate cladding, the present fibers exhibit negligible oxygen despite being fabricated at more than twice the melting point of the germanium. The counterintuitive result of less oxygen when the fiber is drawn at a higher temperatures is discussed. The measured propagation loss for the fiber was 0.7 dB/cm at 3.39 μm, which is the lowest loss reported to date.

Why it matters

OpenAlex reports 61 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Silica-clad optical fibers comprising a core of crystalline germanium were drawn using a molten core technique. With respect to previous fibers drawn using a borosilicate cladding, the present fibers exhibit negligible oxygen despite being fabricated at more than twice the melting point of the germanium. The counterintuitive result of less oxygen when the fiber is drawn at a higher temperatures is discussed. The measured propagation loss for the fiber was 0.7 dB/cm at 3.39 μm, which is the lowest loss reported to date.

Key concepts: Germanium, Materials science, Cladding (metalworking), All-silica fiber, Hard-clad silica optical fiber, Optical fiber, Borosilicate glass, Plastic-clad silica fiber

Related papers

Back to paper searchBrowse research topicsOriginal source
Silica-clad crystalline germanium core optical fibers — Research Paper | ScholarLens