A Preliminary Study of the Carbon-Based Solid Acid Preparation Process

Yong Li Li, Li Ping Mao, Cai Xu, Shi You Li

Open publisher page 1 citations

Abstract

Cotton and sulfuric acid that concentration is 98% as the raw material, to compare the resulting solid carbon sulfonic acid content of the material under different reaction temperatures. FTIR analysis shows that the cotton carbon is an amorphous carbon after sulfonation reactions, a sulfonic acid group present in the resulting material. When the sulfonation temperature is 170 °C, the prepared cotton carbon sulfonic acid has the highest acid content. By the sulfuric acid TG/DTG curve analysis, it verify: 170 °C is the highest activity temperature point of sulfuric acid sulfonation reaction.

About this research paper

What this paper is about

Cotton and sulfuric acid that concentration is 98% as the raw material, to compare the resulting solid carbon sulfonic acid content of the material under different reaction temperatures. FTIR analysis shows that the cotton carbon is an amorphous carbon after sulfonation reactions, a sulfonic acid group present in the resulting material. When the sulfonation temperature is 170 °C, the prepared cotton carbon sulfonic acid has the highest acid content. By the sulfuric acid TG/DTG curve analysis, it verify: 170 °C is the highest activity temperature point of sulfuric acid sulfonation reaction.

Why it matters

OpenAlex reports 1 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Cotton and sulfuric acid that concentration is 98% as the raw material, to compare the resulting solid carbon sulfonic acid content of the material under different reaction temperatures. FTIR analysis shows that the cotton carbon is an amorphous carbon after sulfonation reactions, a sulfonic acid group present in the resulting material. When the sulfonation temperature is 170 °C, the prepared cotton carbon sulfonic acid has the highest acid content. By the sulfuric acid TG/DTG curve analysis, it verify: 170 °C is the highest activity temperature point of sulfuric acid sulfonation reaction.

Key concepts: Sulfuric acid, Sulfonic acid, Raw material, Carbon fibers, Solid acid, Fourier transform infrared spectroscopy, Chemistry, Materials science