EFFECTS OF TEMPERATURE GRADIENT ON LAMEL- LAR ORIENTATIONS OF DIRECTIONAL SOLIDIFIED TiAl-BASED ALLOY

Zhixia Xiao, Zheng Lijing, Lili Yang, Yan Ji, Hu Zhang

Open publisher page 2 citations

Abstract

Directional solidification experiments under heating temperatures of 1580℃and 1650℃were performed on Ti-47Al-2Cr-2Nb alloy in order to obtain the evolution of lamellar grains.Prom microstructural analysis in the mushy zone of directional solidified ingots,βphase was firstly solidified, thenαphase was formed through peritectic reaction;αphase depended on the pre-existedβphase on which it nucleated,and only one of the 12αorientation variants was selected during solid stateβ→αtransformations.As the average temperature gradient of the mushy zone was increased from 40 K/cm to 160 K/cm,the solidification interface morphologies were changed from columnar dendrite to celluar dendrite.Eliminating the influence of cutting plane to theγ-lamella orientation,it was shown that the columnar lamellar grains with an angle of approximately 74°to growth direction gradually overgrew the ones with the angle of nearly 45°to the growth direction at the withdrawal rate of 1 mm/min and temperature gradient of 40 K/cm.Increasing temperature gradient to 160 K/cm,the grains with the angle of about 74°progressively rejected other with the angle of nearly 90°to the growth direction.Calculation of theβdendrite preferred growth orientation indicated thatβdendrites tend to grow along the 110_βorientation at the present solidification experiments.Increasing temperature gradient,the preferred growth tendency ofβdendrite became more drastically,other orientations,such as the 001_βdirectional orientation,could rapidly be replaced.

About this research paper

What this paper is about

Directional solidification experiments under heating temperatures of 1580℃and 1650℃were performed on Ti-47Al-2Cr-2Nb alloy in order to obtain the evolution of lamellar grains.Prom microstructural analysis in the mushy zone of directional solidified ingots,βphase was firstly solidified, thenαphase was formed through peritectic reaction;αphase depended on the pre-existedβphase on which it nucleated,and only one of the 12αorientation variants was selected during solid stateβ→αtransformations.As the average temperature gradient of the mushy zone was increased from 40 K/cm to 160 K/cm,the solidification interface morphologies were changed from columnar dendrite to celluar dendrite.Eliminating the influence of cutting plane to theγ-lamella orientation,it was shown that the columnar lamellar grains with an angle of approximately 74°to growth direction gradually overgrew the ones with the angle of nearly 45°to the growth direction at the withdrawal rate of 1 mm/min and temperature gradient of 40 K/cm.Increasing temperature gradient to 160 K/cm,the grains with the angle of about 74°progressively rejected other with the angle of nearly 90°to the growth direction.Calculation of theβdendrite preferred growth orientation indicated thatβdendrites tend to grow along the 110_βorientation at the present solidification experiments.Increasing temperature gradient,the preferred growth tendency ofβdendrite became more drastically,other orientations,such as the 001_βdirectional orientation,could rapidly be replaced.

Why it matters

OpenAlex reports 2 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Directional solidification experiments under heating temperatures of 1580℃and 1650℃were performed on Ti-47Al-2Cr-2Nb alloy in order to obtain the evolution of lamellar grains.Prom microstructural analysis in the mushy zone of directional solidified ingots,βphase was firstly solidified, thenαphase was formed through peritectic reaction;αphase depended on the pre-existedβphase on which it nucleated,and only one of the 12αorientation variants was selected during solid stateβ→αtransformations.As the average temperature gradient of the mushy zone was increased from 40 K/cm to 160 K/cm,the solidification interface morphologies were changed from columnar dendrite to celluar dendrite.Eliminating the influence of cutting plane to theγ-lamella orientation,it was shown that the columnar lamellar grains with an angle of approximately 74°to growth direction gradually overgrew the ones with the angle of nearly 45°to the growth direction at the withdrawal rate of 1 mm/min and temperature gradient of 40 K/cm.Increasing temperature gradient to 160 K/cm,the grains with the angle of about 74°progressively rejected other with the angle of nearly 90°to the growth direction.Calculation of theβdendrite preferred growth orientation indicated thatβdendrites tend to grow along the 110_βorientation at the present solidification experiments.Increasing temperature gradient,the preferred growth tendency ofβdendrite became more drastically,other orientations,such as the 001_βdirectional orientation,could rapidly be replaced.

Key concepts: Directional solidification, Materials science, Temperature gradient, Lamellar structure, Dendrite (mathematics), Alloy, Phase (matter), Lamella (surface anatomy)

Related papers

Back to paper searchBrowse research topicsOriginal source
EFFECTS OF TEMPERATURE GRADIENT ON LAMEL- LAR ORIENTATIONS OF DIRECTIONAL SOLIDIFIED TiAl-BASED ALLOY — Research Paper | ScholarLens