2003•Unpublished venueRequires access

Aging of Kraft paper in natural ester dielectric fluid

C. Patrick Mcshane, Kevin James Rapp, J.L. Corkran, G.A. Gauger, John Luksich

Open publisher page 88 citations

Abstract

Kraft transformer insulation paper aged in natural ester (vegetable oil) dielectric fluid was compared to identical paper aged in conventional transformer mineral oil. Sealed steel aging tubes containing copper, aluminum, Kraft paper, and dielectric fluid (mineral oil and natural ester) were aged at 150/spl deg/C for 500, 1000, 2000, and 4000 hours. The extent of paper degradation after aging was determined using paper tensile strength, paper degree of polymerization, and furanic compounds in the aged fluid. Water contents of fluids and paper were compared. Paper aged in conventional transformer oil degraded at a significantly faster rate than in natural ester dielectric fluid. Paper in mineral oil reached three criteria for IEEE end-of-life (50% retained tensile strength, 25% retained tensile strength, and degree of polymerization of 200) within the first 1000 hours. After 4000 hours of aging, paper in natural ester did not degrade to any of the IEEE end-of-life criteria. At 4,000 hours, the paper aged in natural ester retained about 55% of the original tensile strength and a degree of polymerization of about 280. Paper aged in conventional transformer oil degraded to the same values in about 315 and 390 hours, respectively-an order of magnitude faster. The reduced paper-aging rate in natural ester is primarily attributed to the fluid maintaining the paper in a very dry state.

About this research paper

What this paper is about

Kraft transformer insulation paper aged in natural ester (vegetable oil) dielectric fluid was compared to identical paper aged in conventional transformer mineral oil. Sealed steel aging tubes containing copper, aluminum, Kraft paper, and dielectric fluid (mineral oil and natural ester) were aged at 150/spl deg/C for 500, 1000, 2000, and 4000 hours. The extent of paper degradation after aging was determined using paper tensile strength, paper degree of polymerization, and furanic compounds in the aged fluid. Water contents of fluids and paper were compared. Paper aged in conventional transformer oil degraded at a significantly faster rate than in natural ester dielectric fluid. Paper in mineral oil reached three criteria for IEEE end-of-life (50% retained tensile strength, 25% retained tensile strength, and degree of polymerization of 200) within the first 1000 hours. After 4000 hours of aging, paper in natural ester did not degrade to any of the IEEE end-of-life criteria. At 4,000 hours, the paper aged in natural ester retained about 55% of the original tensile strength and a degree of polymerization of about 280. Paper aged in conventional transformer oil degraded to the same values in about 315 and 390 hours, respectively-an order of magnitude faster. The reduced paper-aging rate in natural ester is primarily attributed to the fluid maintaining the paper in a very dry state.

Why it matters

OpenAlex reports 88 citations for this work. Citation counts describe recorded attention and do not establish research quality.

Key contribution

A contribution statement is not available in the OpenAlex record.

Method / approach

Method details are not available in the OpenAlex metadata.

Main findings

Findings are not separately available in the OpenAlex metadata.

Limitations

Limitations are not available in the OpenAlex metadata.

Applications

Application details are not available in the OpenAlex metadata.

Available abstract

Kraft transformer insulation paper aged in natural ester (vegetable oil) dielectric fluid was compared to identical paper aged in conventional transformer mineral oil. Sealed steel aging tubes containing copper, aluminum, Kraft paper, and dielectric fluid (mineral oil and natural ester) were aged at 150/spl deg/C for 500, 1000, 2000, and 4000 hours. The extent of paper degradation after aging was determined using paper tensile strength, paper degree of polymerization, and furanic compounds in the aged fluid. Water contents of fluids and paper were compared. Paper aged in conventional transformer oil degraded at a significantly faster rate than in natural ester dielectric fluid. Paper in mineral oil reached three criteria for IEEE end-of-life (50% retained tensile strength, 25% retained tensile strength, and degree of polymerization of 200) within the first 1000 hours. After 4000 hours of aging, paper in natural ester did not degrade to any of the IEEE end-of-life criteria. At 4,000 hours, the paper aged in natural ester retained about 55% of the original tensile strength and a degree of polymerization of about 280. Paper aged in conventional transformer oil degraded to the same values in about 315 and 390 hours, respectively-an order of magnitude faster. The reduced paper-aging rate in natural ester is primarily attributed to the fluid maintaining the paper in a very dry state.

Key concepts: Kraft paper, Mineral oil, Electrical insulation paper, Ultimate tensile strength, Composite material, Materials science, Transformer oil, Transformer

Related papers

Back to paper searchBrowse research topicsOriginal source
Aging of Kraft paper in natural ester dielectric fluid — Research Paper | ScholarLens