CdS thin films have been prepared by chemical bath deposition (CBD) method on glass substrates at solution temperature 80 o C. Cadmium acetate was used as a source of Cd + 2 and thiourea as a source S -2 . After three times of sequences deposition a 100 nm CdS thin films is obtained. The Structure of these films studied by X-Ray diffraction were polycrystalline hexagonal phase. The films exhibited high optical transmittance T~50-100 % and low reflectance in the wavelength (500-900)nm which make them useful as a transparent window in solar cells. The optical constants (n,k) were also calculated in the same spectrum region. The optical transitions were due to direct allowed in quantum mechanical sense. The value of the optical energy gap for the as deposited and annealed films was in the range (2.35-2.43) eV. Vacuum annealing at (200,300) o C improved the crystalline structure of the
OpenAlex reports 40 citations for this work. Citation counts describe recorded attention and do not establish research quality.
A contribution statement is not available in the OpenAlex record.
Method details are not available in the OpenAlex metadata.
Findings are not separately available in the OpenAlex metadata.
Limitations are not available in the OpenAlex metadata.
Application details are not available in the OpenAlex metadata.
CdS thin films have been prepared by chemical bath deposition (CBD) method on glass substrates at solution temperature 80 o C. Cadmium acetate was used as a source of Cd + 2 and thiourea as a source S -2 . After three times of sequences deposition a 100 nm CdS thin films is obtained. The Structure of these films studied by X-Ray diffraction were polycrystalline hexagonal phase. The films exhibited high optical transmittance T~50-100 % and low reflectance in the wavelength (500-900)nm which make them useful as a transparent window in solar cells. The optical constants (n,k) were also calculated in the same spectrum region. The optical transitions were due to direct allowed in quantum mechanical sense. The value of the optical energy gap for the as deposited and annealed films was in the range (2.35-2.43) eV. Vacuum annealing at (200,300) o C improved the crystalline structure of the
Key concepts: Chemical bath deposition, Thin film, Crystallite, Materials science, Transmittance, Annealing (glass), Band gap, Analytical Chemistry (journal)